HCl + AgNO3 = HNO3 + AgCl : How?
I mixed aqueous Hydrochloric Acid with aqueous Silver Nitrate, and got a precipitate of Silver Chloride, so I knew there was Nitric Acid present.
My understanding was that an acid used must be stronger to convert a salt to it's acid, is this not correct?
"Damn it George! I told you not to drop me!"
|
|
DJF90
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline
Mood: No Mood
|
|
That is correct. HCl is about 6 orders of magnitude stronger than nitric acid. You've also got the precipitation of insoluble silver chloride as a
driving factor. So wheres the problem?
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
Wow! I thought Nitric was stronger! Thanks.
"Damn it George! I told you not to drop me!"
|
|
bismuthate
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline
Mood: self reacting
|
|
Kind of on the subject why does HNO3 react with AlCl3? I know that HCl is stronger.
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
From what I understand, in that case it's a matter of being a strong oxidizer, rather than a stronger acid. The Aluminium Chloride is oxidized to
Nitrosyl Chloride and Aluminium Nitrate, which I belive relies off of a different mechanism.
"Damn it George! I told you not to drop me!"
|
|
bismuthate
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline
Mood: self reacting
|
|
Ok that makes more sense thanks. Also, how does S replace Cl when H2S passes through CuCl? Sorry for all the questions.
|
|
barley81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 481
Registered: 9-5-2011
Member Is Offline
Mood: No Mood
|
|
Cu2S is very insoluble. Ksp = 2.5 x 10^(-48) (http://www.csudh.edu/oliver/chemdata/data-ksp.htm)
CuCl is not that insoluble. Ksp = 1.2 x 10^(-6).
Consider saturated CuCl. Since [Cu+] = [Cl-], we have x^2 = 1.2 x 10^-6 and x = [Cu+] = 1.1 x 10^-3 M.
Consider 0.1M H2S: K<sub>1</sub> = 9.6 x 10^-8 and K2 = 1.3 x 10^-14. Now K1 = [H+][HS-]/[H2S] and K2 = [H+][S2-]/[HS-], so K1K2 =
[H+]^2[S2-]/[H2S]. [H+] is roughly 10^-3, so [S2-] is roughly 1.3 x 10^-15.
If these are in the same solution, then [S2-][Cu+]^2 = 1.5 x 10^-21, which is greater than Ksp for Cu2S. Therefore Cu2S will precipitate.
EDIT: metalresearcher is right. It does not have anything to do with acid strength, though acid strength can influence things indirectly. For example,
insoluble metal carbonates dissolve in acid because the carbonate ion is protonated as soon as it dissolves, and the CO2 is driven off. Therefore Qsp
remains below Ksp, and the solid can continue dissolving.
[Edited on 18-11-2013 by barley81]
|
|
metalresearcher
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 737
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
Well it has nothing to do with acid strength. HCl and AgNO3 in an aqueous solution *will* precipitate AgCl as Ag+ and Cl- ions cannot co-exist in an
aqueous solution due to its very poor solubility.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Those acquainted with hydrometallury are acquainted with the use of Citric acid as an apparently more effective, cheaper and environmentally more
friendly leaching lixiviant. To quote a recent source (August 2011, Volume 13, Issue 2, Journal of Material Cycles and Waste Management, pp 118-126,
"Leaching of heavy metals by citric acid from fly ash generated in municipal waste incineration plants", by Kai Huang,.. at http://link.springer.com/article/10.1007%2Fs10163-011-0001-5... ):
"From the results of screening tests of leaching lixiviants, citric acid was found to be the most effective leaching agent"
This is quite an interesting statement as among the competing lixiviants where the inorganic acids HCl, H2SO4 and even HNO3.
I will let the student do research to undercover the explanation.
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
Metalresearcher, I think it does have to do with acid strength. If HCl wasn't strong enough to react with AgNO3, no reaction would occur, thus no
precipitate.
"Damn it George! I told you not to drop me!"
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | Those acquainted with hydrometallury are acquainted with the use of Citric acid as an apparently more effective, cheaper and environmentally more
friendly leaching lixiviant. To quote a recent source (August 2011, Volume 13, Issue 2, Journal of Material Cycles and Waste Management, pp 118-126,
"Leaching of heavy metals by citric acid from fly ash generated in municipal waste incineration plants", by Kai Huang,.. at http://link.springer.com/article/10.1007%2Fs10163-011-0001-5... ):
"From the results of screening tests of leaching lixiviants, citric acid was found to be the most effective leaching agent"
This is quite an interesting statement as among the competing lixiviants where the inorganic acids HCl, H2SO4 and even HNO3.
I will let the student do research to undercover the explanation.
|
Citric acid is a very effective lixiviant because it is a complexing agent as well as an acid.
Look at Benedict's Solution, the copper is complexed by the .citrate anion.
http://en.wikipedia.org/wiki/Benedict%27s_reagent
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by ScienceSquirrel ![](images/xpblue/lastpost.gif) | Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | Those acquainted with hydrometallury are acquainted with the use of Citric acid as an apparently more effective, cheaper and environmentally more
friendly leaching lixiviant. To quote a recent source (August 2011, Volume 13, Issue 2, Journal of Material Cycles and Waste Management, pp 118-126,
"Leaching of heavy metals by citric acid from fly ash generated in municipal waste incineration plants", by Kai Huang,.. at http://link.springer.com/article/10.1007%2Fs10163-011-0001-5... ):
"From the results of screening tests of leaching lixiviants, citric acid was found to be the most effective leaching agent"
This is quite an interesting statement as among the competing lixiviants where the inorganic acids HCl, H2SO4 and even HNO3.
I will let the student do research to undercover the explanation.
|
Citric acid is a very effective lixiviant because it is a complexing agent as well as an acid.
Look at Benedict's Solution, the copper is complexed by the .citrate anion.
http://en.wikipedia.org/wiki/Benedict%27s_reagent |
Yes, Citric acid complexing ability is usually cited.
The acid's solubility (related no doubt to its ability to form complexes) is another plus. The dry acid does not decompose until heated over 300 C
(good thermal stability). Also, an aqueous solution of Critic acid is less volatile (or harder to be boiled off) probably adds to its performance as
an effective lixiviant.
[Edited on 19-11-2013 by AJKOER]
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by APO ![](images/xpblue/lastpost.gif) | Metalresearcher, I think it does have to do with acid strength. If HCl wasn't strong enough to react with AgNO3, no reaction would occur, thus no
precipitate. |
I don't think that's quite correct, because everything is dissociated in solution. When you mix a solution of hydrochloric acid and silver nitrate,
you get a soup containing H3O+, Cl-, Ag+, and NO3-. The silver and chloride ions
very readily combine to form a precipitate of AgCl because it is nearly insoluble in solution. This is the main driver of the reaction, and leaves
H3O+ and NO3- in solution to form nitric acid. If done stroichiometrically, I would think this should
yield quite pure, or at least chloride-free, acid!
|
|
APO
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 627
Registered: 28-12-2012
Location: China Lake
Member Is Offline
Mood: Refluxing
|
|
Oh, thanks. It would be different with a covalent bond correct?
"Damn it George! I told you not to drop me!"
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
I think so, yes. If, say, HCl wasn't dissociated then the chlorine atom would be less readily available to bond to a silver atom.
Thinking about all this, I know less about covalent bonds than I thought I did. I'll look into it more, and if I'm incorrect please someone correct
me.
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Quote: |
I think so, yes. If, say, HCl wasn't dissociated then the chlorine atom would be less readily available to bond to a silver atom.
|
If HCl was covalently bonded, it wouldn't be an acid.
HCl is a stronger acid than HNO3 so it will liberate HNO3 from nitrate salts.
In the case that HCl would be a weaker acid than HNO3, this reaction could still be possible because of the very low solubility of the
AgCl. Then you would have to compare the Ksp with the Ka.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
Dany
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 482
Registered: 3-8-2013
Member Is Offline
Mood: No Mood
|
|
if HCl were in the gas phase (not dissociated) you wouldn't call it acid???
Saying that if HCl was covalently bonded, it wouldn't be an acid is not true. another example is the active hydrogen compounds like malonate esters.
in the presence of base they will act as acid by giving the covalently bonded hydrogen forming the enolate form which is useful in organic synthesis,
or for example the formation of acetylide from acetylene when reacted with liquid ammonia at -33°C.
I will add one more thing. The concept of acid and bases is relative. Even nitric acid will act as a base when mixed with sulfuric acid (because the
pKa of H2SO4 is less than the HNO3) which will lead to the protonation of nitric acid and the formation of the
nitronium cation (NO2+) after the elimination of water molecule.
so depending on the situation a species may act as an acid or base
Dany.
[Edited on 22-11-2013 by Dany]
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Generally I classify acids as acids when they are capable of protonating water. I find this a useful distinction in most situations, but you are
right, in different media the lines are blurred.
Quote: |
if HCl were in the gas phase (not dissociated) you wouldn't call it acid???
|
You are right, I was wrong.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|