[*] posted on 26-1-2013 at 19:59
recovery of polymer from solution


anti-solvent for chlorobenzene;);)
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 27-1-2013 at 02:10


Depends on the polymer.
View user's profile View All Posts By User
Nicodem
Super Moderator
Thread Moved
27-1-2013 at 07:23
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 1-2-2013 at 18:27


Rotovap off the chlorobenzene. Use your mouth on the vacuum outlet and suck in, inhaling deeply, to reduce the system pressure. When consciousness is regained, check for remaining solvent, and repeat as necessary until you're left with pure polymer.



View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 1-2-2013 at 21:59


Quote: Originally posted by bfesser  
Rotovap off the chlorobenzene. Use your mouth on the vacuum outlet and suck in, inhaling deeply, to reduce the system pressure. When consciousness is regained, check for remaining solvent, and repeat as necessary until you're left with pure polymer.


Well, let's not advocate suicide by stupidity just yet.

Dear hossein0591,

You've started more than 5 threads on this same subject. The fact that no one has helped you so far likely means that the answer lies within your grasp; if you'd care to do a simple search, or tell us what polymer you're working with and how you wish to extract it.

Either give us some more information than "anti-solvent for chlorobenzene" (the hell is an anti-solvent?), or work it out for yourself.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 859
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 1-2-2013 at 22:23


Quote: Originally posted by elementcollector1  
(the hell is an anti-solvent?)

It's a solvent (in which the desired product is insoluble) which you add to a solution to cause precipitation. Try to add acetone to a solution of table salt.




This just in: 95,5 % of the world population lives outside the USA
You should really listen to ABBA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User
Nicodem
Super Moderator
*******




Posts: 4230
Registered: 28-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 2-2-2013 at 02:33


Quote: Originally posted by Lambda-Eyde  
Quote: Originally posted by elementcollector1  
(the hell is an anti-solvent?)

It's a solvent (in which the desired product is insoluble) which you add to a solution to cause precipitation. Try to add acetone to a solution of table salt.

Your definition is fine, but acetone and solutions of table salt do not mix in all proportions. In many combinations, all you get is a biphasic (liquid-liquid) or a triphasic mixture (liquid-liquid-solid), so it is not the best example. The phrase "antisolvent" is commonly used in crystallization process development (for example, in the pharmaceutical industry, but also elsewhere).




…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)