A way to chemically remove lead oxide


Today I found some old lead. I tried lots of ways of chemically removing the dull oxide layer to reveal the shiny metal itself. But it did not work. I tried:
.Boiling in NaHSO4 solution
.Boiling in NaOH solution (concentrated)
.Boiling in dilute nitric acid (obviously because the nitric acid was oxidizing, it could not work)
Finally I gave up, and just melted it and poured it out.
But melting leaves a lot of residues (lead+oxides of lead on the inside of the (metal) container. Is there a way to remove the oxide layer chemically? From the searches on the internet, it appears that HCl and cold alkali metal hydroxide solutions will, over time. But I want to confirm this+see if there is any other quicker ways.

Also, I haven't got mineral oil or de oxygenated water right now. Would storing the shiny lead in a NaCl solution (displaces oxygen out of water) be able to prevent it from going dull again?
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 20-3-2012 at 08:13


Quote: Originally posted by weiming1998  
Is there a way to remove the oxide layer chemically?
Acetic acid. See the two lead acetate pages on Wikipedia. I haven't tried it personally, as I don't want to deal with soluble Pb.
View user's profile View All Posts By User
arsphenamine
Hazard to Others
***




Posts: 236
Registered: 12-8-2010
Location: I smell horses, Maryland, USA
Member Is Offline

Mood: No Mood

[*] posted on 20-3-2012 at 13:38


Lead salts may be precipitated as PbSO<sub>4</sub> with sulfuric acid.
Ksp is around 10<sup>-8</sup>.
View user's profile View All Posts By User