andra
Harmless
Posts: 13
Registered: 16-9-2011
Member Is Offline
Mood: No Mood
|
|
solubilizing phthalates
In what can I solubilize chitosan-phthalate? or just phthalates?? Because it seems that is not soluble in acetic acid and water, nor in DMSO, nor in
methanol or chloroform. I need it in order to do the NMR analysis.
Thanks!
Andra.
|
|
ThatchemistKid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 2-6-2010
Member Is Offline
|
|
I am not sure about dissolving your chitosan-phthalate considering it has that large amino sugar polymer group on it, but the NMR spectra of
chitosan-phthalate will be completely different from just "any phthalate"
para-phthalaic acid is I believe slightly soluble in methanol or ethanol from which it is recrystallized generally, also the phthalate ester is
soluble in its corresponding alcohol for the ethyl and methyl esters, probably also soluble in acetone. Do you have any d5-acetone or deuterated
alcohols in your NMR lab that you can use as solvents...what exactly are you trying to work with it was a little unclear. Also what is the strength of
your NMR's magnet?
[Edited on 29-9-2011 by ThatchemistKid]
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
Phthalate esters dissolve very well in methanol. We used to see them extracted from plastics frequently when people used certain plastic containers
to hold solvent or samples for NMR.
If you are desperate, you could try TFA or a mix of DMSO, methanol and CDCl3. Chitosan is not exactly a small molecule.
Bob
|
|
Ozone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
My old research group used phthalic anhydride to add a low degree of substitution to disrupt the crystallinity of the material in order to get it into
solution. You may have over-substituted (or cross-linked--in this case your screwed) it. Have you tried toluene?
Did your material ppt in brine?
O3
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|
Nicodem
Super Moderator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
What is "chitosan-phthalate"? Is that a phthalate salt of chitosan? An ester? An amide? Is it fully functionalized, partially or what? What do
"phthalates" in general have to do with your question? What makes you think other people can read your mind?
PS: Please open unanswerable and/or referenceless threads only in the Beginnings section where I'm moving this.
|
|
Nicodem
|
Thread Moved 1-10-2011 at 01:37 |
Ozone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline
Mood: Integrated
|
|
Phthalimides... If everything goes well.
Here are a couple of citatations (I was from the Daly group and did a lot of the early modifications of Chitosan via reductive amination, etc.)
Besides the attached, see also:
1: Sajomsang W, Tantayanon S, Tangpasuthadol V, Daly WH. Quaternization of N-aryl
chitosan derivatives: synthesis, characterization, and antibacterial activity.
Carbohydr Res. 2009 Dec 14;344(18):2502-11. Epub 2009 Sep 30. PubMed PMID:
19863950.
2: Sajomsang W, Tantayanon S, Tangpasuthadol V, Thatte M, Daly WH. Synthesis and
characterization of N-aryl chitosan derivatives. Int J Biol Macromol. 2008 Aug
15;43(2):79-87. Epub 2008 Apr 15. PubMed PMID: 18514305.
3: Zhang C, Price LM, Daly WH. Synthesis and characterization of a trifunctional
aminoamide cellulose derivative. Biomacromolecules. 2006 Jan;7(1):139-45. PubMed
PMID: 16398508.
Cheers,
O3
Attachment: Daly et al 2010.pdf (412kB) This file has been downloaded 951 times
Attachment: Kurita et al 2002 Biomacromol. 3 (1), pp 1-4.pdf (81kB) This file has been downloaded 515 times
-Anyone who never made a mistake never tried anything new.
--Albert Einstein
|
|