tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2008 at 11:19
CuCl2.H2O to powder?


Ok so I've been lurking around for a while and I have a question.
I've taken 60ml of H2O2 (3% Peroxide)
and 30ml HCL (Muratic Acid 31.??%)
and added some copper wire (inside of Coax cable)
Stirred magnetically on stir plate until all copper was dissolved
I presume now it is CuCl2.H2O
How would I make it into powdered form?
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8027
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 11-11-2008 at 11:38


You don't have CuCl2.H2O, but you do have copper(II) ions and chloride ions in solution (plus a lot of other stuff, like H(+), Cl2, excess H2O2, etc.).

Making solid CuCl2.2H2O can be done by heating the liquid, until most of the liquid is driven off. Make a syruppy liquid, but don't boil to dryness. Heating too much will cause loss of HCl and you'll end up with a basic chloride.

The syrup then can be put on a heat radiator (60 C or so) for a few days and then crystals of CuCl2.2H2O will separate. The product you'll get most likely will become grass-green with a brownish hue. This is because some HCl may remain in the product. Really pure CuCl2.2H2O is not green, but cyan (green/blue).



It also differs a lot from copper sulfate, which is much more blue:



With these two images you should be able to assess the purity of your sample and you see the difference with the sulfate very nicely.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2008 at 12:12


Quote:
Originally posted by woelen
You don't have CuCl2.H2O, but you do have copper(II) ions and chloride ions in solution (plus a lot of other stuff, like H(+), Cl2, excess H2O2, etc.).
Copper chloride exists in two forms in solution, as either/both Cu(I) and Cu(II) ions. This is a commercial etchant for printed circuit boards. The basic reaction is Cu<sup>0</sup> + Cu<sup>2+</sup> --> 2 Cu<sup>+</sup>. So there's CuCl<sub>2</sub> in solution only if the copper ion is completely oxidized. If you want it completely oxidized, you can bubble air through it, or more quickly, pour an excess of H<sub>2</sub>O<sub>2</sub> in. There's quite a good treatment of this as an etchant here: http://members.optusnet.com.au/~eseychell/PCB/etching_CuCl/i...
View user's profile View All Posts By User
tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2008 at 13:20


so when i get home ill give it a shot this drying a shot, ill boil it at 100c until it is syrupy (is that a word?) then i should reduce heat to 60c until it crystalizes. please correct me if im wrong
View user's profile View All Posts By User
kilowatt
Hazard to Others
***




Posts: 322
Registered: 11-10-2007
Location: Montana
Member Is Offline

Mood: nitric

[*] posted on 11-11-2008 at 19:03


The first step will be to filter out any CuCl, which is an insoluble white powder that forms with excess copper in CuCl2.

Then, what's wrong with just heating it strongly in a distillation apparatus until anhydrous CuCl2 (a brown solid that easily breaks into powder/dust) is formed? Anhydrous CuCl2 left out in the air for a few hours or days will absorb moisture to form CuCl2*2H2O.

[Edited on 11-11-2008 by kilowatt]

HPIM1434.JPG - 123kB




The mind cannot decide the truth; it can only find the truth.
View user's profile View All Posts By User
tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 12-11-2008 at 10:19


well so far not so good
here is what it looked like this morning before i went to work







3 hours later i went home to lunch and it was crystals
black in the center then brown to light green to dark green with liquid in it still
I threw out the black and mixed the rest up added more H2O2 and then warmed until it was brown and light green
scraped it up and put it in an open container.
Hopefully tonight it will start looking right

[Edited on 12-11-2008 by tom_servo]

[Edited on 12-11-2008 by tom_servo]
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8027
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 12-11-2008 at 11:03


If you have black stuff in it, then not all copper was oxidized to the +2 oxidation state. Black material is an indication of a mix of copper(I) and copper(II) species, such a mix forms very dark mixed-oxidation-state complexes.

So, redissolve in HCl and add a little more H2O2 and repeat.

@kilowatt: Simply heating is not good. You will suffer from loss of HCl and you get contamination with a mixed oxide/chloride:

CuCl2.2H2O --> Cu(Cl2/O) + H2O + HCl (not balanced, exact stoichiometry cannot be given, depends on temperature).

The mixed chloride/oxide of copper(II) has a green color when it still has water in it, it is very dark brown when anhydrous. You can easily see if your sample has oxide contamination. A solution of the material (either green or dark brown does not matter) in distilled water then remains somewhat turbid. Oxide-free CuCl2.2H2O or CuCl2 gives a perfectly clear green/cyan/blue solution, the exact color depending on concentration.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 13-11-2008 at 07:02


so i added some peroxide and now it is a lighter green.
I added just a tad and stirred it up, I guess ill let it evaporate for a few days and see what happens
View user's profile View All Posts By User
tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-11-2008 at 07:18


medium green crystals
Ill take a picture this weekend and post it
even if it is not what i was looking for its beautiful
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8027
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 14-11-2008 at 13:00


Add a small amount of your green material to water. Do you get a clear green/blue solution, or does it remain somewhat turbid? If it becomes perfectly clear, then you have done a fairly good job. The green color (and not cyan) probably is due to some remaining HCl and excess water. Copper(II) forms all kinds of complexes and you easily obtain CuCl2.xHCl.yH2O with x and y of indeterminate value (x probably quite small).



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
tom_servo
Hazard to Self
**




Posts: 52
Registered: 11-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-11-2008 at 13:25


it become a light green liquid almost looks like cartoon version of toxic waste or Ghostbusters Hi-C Etco cooler
View user's profile View All Posts By User