[*] posted on 6-7-2007 at 10:49
Anything fun to do with Aluminum Chloride


I believe its the hydrated form.

Any cool color changes or what not with things lying around the house?
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8069
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 6-7-2007 at 13:26


Aluminium chloride hexahydrate is not that interesting. You can make precipitates of Al(OH)3 with it, which redissolve on adding more base, forming aluminates. Adding acid again produces the precipitate again, which redissolves on adding more acid.

The hydrate is not really suitable as an aid in organic syntheses, for that purpose the anhydrous solid is used.

Aluminium chloride has one interesting effect, it has a deodorizing effect, and as such, a dilute solution of this compound can be used.

Making colorful precipitates with aluminium ions is not easy. The ion is colorless, and in precipitates it does not add to the color. As long as the anion in the precipitate is colorless, the precipitate will be white. With ferricyanides and ferrocyanides you can obtain colored precipitates, but these are due to the color of the anion.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Nerro
National Hazard
****




Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline

Mood: Whatever...

[*] posted on 6-7-2007 at 14:12


Does it fume when you put water on it? If it doesn't it is the hydrated form and it's pretty much useless.

[Edited on 6-7-2007 by Nerro]




#261501 +(11351)- [X]

the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally

courtesy of bash
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 6-7-2007 at 14:24


I have some of what I recall is hexahydroaluminum chloride, which dried to yellowish crystals which eventually became gooey (amorphous, I would suspect) and yellow-orange.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
cbfull
Harmless
*




Posts: 33
Registered: 24-6-2006
Location: OH
Member Is Offline

Mood: No Mood

[*] posted on 2-8-2007 at 19:03


If you make a 20% solution in anhydrous ethanol you have a prescription strength antiperspirant.
View user's profile View All Posts By User
Nerro
National Hazard
****




Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline

Mood: Whatever...

[*] posted on 2-8-2007 at 22:12


Yeah how does that work?!



#261501 +(11351)- [X]

the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally

courtesy of bash
View user's profile View All Posts By User
YT2095
International Hazard
*****




Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline

Mood: within Nominal Parameters

[*] posted on 3-8-2007 at 06:14


if you get a hot enough burning composition (a perchlorate), you should be able to use it as a chlorine donor in strobe effect stars.



\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5134
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 3-8-2007 at 16:35


I'm not sure that answers this question "Yeah how does that work?! "
in this context "If you make a 20% solution in anhydrous ethanol you have a prescription strength antiperspirant" unles you have pyrotechnic armpits on a regular basis.
View user's profile View All Posts By User
Ozone
International Hazard
*****




Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline

Mood: Integrated

[*] posted on 3-8-2007 at 16:42


I don't know how fun it is, but...

Hydrated AlCl3 is an excellent coagulant for cloudy water, etc. It can be used to clarify most aqueous samples including river water, sewage, cane juice, etc. See poly aluminum chloride (PAC).

Cheers,

O3

[Edited on 3-8-2007 by Ozone]




-Anyone who never made a mistake never tried anything new.
--Albert Einstein
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 3-8-2007 at 20:03


And also a mordant (when neutralized, gives floc of Al(OH)3 which absorbs dyes well).

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
YT2095
International Hazard
*****




Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline

Mood: within Nominal Parameters

[*] posted on 4-8-2007 at 05:38


Quote:
Originally posted by unionised
I'm not sure that answers this question "Yeah how does that work?! "
in this context "If you make a 20% solution in anhydrous ethanol you have a prescription strength antiperspirant" unles you have pyrotechnic armpits on a regular basis.


because I wasn`t addressing that, I was addressing the OP, if you scroll up to the top you`ll see "Anything fun to do with Aluminum Chloride?" was asked.
That`s what I was addressing :)




\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
View user's profile View All Posts By User
organometallic
Hazard to Self
**




Posts: 53
Registered: 22-7-2007
Location: United Kingdom
Member Is Offline

Mood: No Mood

[*] posted on 4-8-2007 at 16:57


Can be used in various organic reactions..Not sure If you will consider these fun exactly, but it can be used to catalyse friedal-crafts reactions, useful in polymerisation and isomerisation of various hydrocarbons. It can also be used to introduce aldehyde groups onto aromatic rings (benzaldehyde, anyone?).
-mostly from wikipedia.




In vials of ivory and coloured glass
Unstoppered, lurked her strange synthetic perfumes,
Unguent, powdered, or liquid - troubled, confused
And drowned the sense in odours.
View user's profile View All Posts By User
Nerro
National Hazard
****




Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline

Mood: Whatever...

[*] posted on 4-8-2007 at 17:08


That only works with anhydrous AlCl3 and not with [Al(H<sub>2</sub>O)<sub>6</sub>]Cl<sub>3</sub>



#261501 +(11351)- [X]

the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally

courtesy of bash
View user's profile View All Posts By User
Nicodem
Super Moderator
*******




Posts: 4230
Registered: 28-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 4-8-2007 at 23:13


Quote:
Originally posted by organometallic
Can be used in various organic reactions..

There is no use for it in organic reactions that I know of and I'm an organic chemist so I should know. As Nerro indicates you obviously confused it with AlCl3 which is a strong acid used to enhance many electrophiles and activate some proelectrophiles for many types of reactions (including Friedel-Crafts reactions). But [Al(H2O)6]Cl3 is a weak acid and is completely useless as such.




…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)