Pages:
1
2 |
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
I ran a quick qualitative experiment to test out the possibility of making AlCl3 in methanol. Freshly dried anhydrous CuCl2 was
dissolved in dry methanol (dried over anhydrous MgSO4). A crumpled piece of aluminum foil was added to the solution (left). To compare,
some of the same CuCl2 was added to another beaker containing water (right), and a piece of aluminum foil was added to it as well.
Effervescence was observed in the methanol solution. After a few minutes without much happening, a small grain of iodine was added to each beaker.
This did not appear to change anything- a slight increase in the rate of effervescence at best.
Displaced copper metal was observed in both solutions, but was evolved more rapidly in the aqueous solution. Effervescence was observed in both
solutions but occurred at a much faster rate in the methanolic solution.
![Methanol-CuCl2.JPG - 1.1MB](http://www.sciencemadness.org/talk/files.php?pid=509529&aid=65751)
I don't think that these conditions will work for producing AlCl3, but it is difficult to determine what is actually happening here.
Aluminum methoxide forming in situ?
|
|
clearly_not_atara
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2723
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
Copper is known to activate aluminium (usually CuSO4) so the methoxide seems like a strong possibility.
Iodine reacts rapidly with methanol and cannot be used to activate aluminium in methanol. Formaldehyde is produced. Solvents compatible with I2
include acetonitrile, propylene carbonate, tert-butanol (maybe) and DMF. Acetone will surely be oxidized; DMSO might be oxidized.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Iodine reacts rapidly with methanol? I don't think so- I've run labs where the students react iodine with zinc in dry methanol to determine the
product of the reaction.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
clearly_not_atara
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2723
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
Really? I suppose I was wrong. I2 has come up for alcohol oxidations before, can't remember why.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
In basic solution, iodine will oxidize things like isopropanol to give acetone, and then follow up with the iodoform reaction, but we've boiled zinc
and iodine in methanol for extended periods without the methanol obviously reacting.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Not to mention using iodine and phosphorus (or aluminum!) in methanol or ethanol to make the corresponding iodides. It's pretty well accepted that
iodine does not oxidize methanol to formaldehyde.
[Edited on 3-6-2018 by Texium (zts16)]
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Oh, and last night after about an hour, the aluminum fully reacted with the methanolic CuCl2 (solution was colorless, copper metal and
excess aluminum was present). The aqueous solution took much less time to react.
I decided to test the methanolic solution by adding a few drops to a test tube with some water. It didn't visibly react, but the mixing was noticeably
exothermic. It seems most likely that there is dissolved aluminum methoxide present, as there wasn't any HCl gas formed as far as I could tell. In
retrospect I suppose I should have checked the pH, but I wasn't really thinking.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Why would you even consider the formation of methoxide? The expected product would be aluminum chloride, solvated with methanol.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Do you know for a fact that aluminum chloride doesn't react with methanol? I couldn't find anything saying explicitly that it does or doesn't, but I
also saw that aluminum chloride generally reacts with alcohols to give alkoxides: https://www.masterorganicchemistry.com/2011/07/22/reagent-fr... (Yeah, I know it's a homework-helping site so take it for what it's worth)
And while looking around I also saw this patent: https://patents.google.com/patent/US3083218
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
I would expect the equilibrium of AlCl3 + 3 ROH = Al(OR)3 + 3 HCl to lie to the left, because methoxide is a really strong base (even when coordinated
to aluminum) and HCl is a really strong acid. If you were to boil off the HCl, you might get the methoxide, but I'd guess you'd be more likely to get
a crappy mix of oxide, hydroxide, methoxide and basic chloride.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Pages:
1
2 |