First up, I'm just going to put it out there that this is my first post, so soz in advance if I accidentally post in the wrong thread or something
else like that (:
So, I want to make some nice green flames for the family in conjunction with the red strontium flames I'm making (it's the whole "red and green"
Christmas theme). I've got some borax (aka sodium borate or disodium tetraborate Na2B4O7) that allegedly burns green when prepared properly.
According to my knowledge, the sodium cation in borax causes borax to normally burn yellow when dissolved in water. However, upon adding methanol
(CH3OH), trimethyl borate is formed. The prescence of the borate ion turns the flame green during combustion.
Now, I'm having difficulty finding methanol, but I have frequently found methylated spirits being sold in my area. According to what I've searched up,
methylated spirits are virtually just 10% methanol and 90% ethanol, so this stuff contains two types of alkanols that should react with borax. My
question here is, can methylated spirits be substituted with methanol in mixing borax to produce green flames, or does the ethanol somehow not work?
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Online
Mood: Semi-victorious.
|
|
I seem to recall that you need to add a bit of sulphuric acid to get the borax/ethanol mixture to work.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
You get better results with boric acid than you do with borax. No sodium ion to get in the way.
Making boric acid from borax is quite straightforward: mix up a solution of borax at high temperature to get a nice concentrated solution. Add some
concentrated hydrochloric acid and watch your boric acid precipitate out. Filtering it while it is still warm is ok and lessens the liklihood of
retaining some crystallised borax (which will occur on cooling.)
Adding this to either methanol or ethanol will work -- you get methyl borate or ethyl borate but both burn green. Using methanol is preferred since
there is less carbon to add yellow to the flame.
If you need it, methanol is sold in the US as a Heet product. (I can't remember what its intended use is.
I tried this last year at Christmas. My problem actually was getting somethig strontium based that have a nice continuous flame.
|
|
goldensquid2000
Harmless
Posts: 3
Registered: 18-12-2017
Member Is Offline
Mood: No Mood
|
|
Wait, really? The problem is that I live in Australia, where the stuff is heavily regulated. Can any other acids be substituted?
|
|
goldensquid2000
Harmless
Posts: 3
Registered: 18-12-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | You get better results with boric acid than you do with borax. No sodium ion to get in the way.
Making boric acid from borax is quite straightforward: mix up a solution of borax at high temperature to get a nice concentrated solution. Add some
concentrated hydrochloric acid and watch your boric acid precipitate out. Filtering it while it is still warm is ok and lessens the liklihood of
retaining some crystallised borax (which will occur on cooling.)
Adding this to either methanol or ethanol will work -- you get methyl borate or ethyl borate but both burn green. Using methanol is preferred since
there is less carbon to add yellow to the flame.
If you need it, methanol is sold in the US as a Heet product. (I can't remember what its intended use is.
I tried this last year at Christmas. My problem actually was getting somethig strontium based that have a nice continuous flame.
|
Thanks for the advice. I'm not too fussy with some yellow in my flame, but the boric acid conversion sounds like an idea to try. Luckily, HCL is
available in Oz, so I'll be able to get some. I might use a coffee filter for the boric acid, since regular filter paper is a pain to get here.
With the methanol/ethanol thing, I don't really have much of a choice unfortunately, since methanol is apparently regulated in Oz and not available
for commercial use. I don't mind though, since a little yellow will make the flame seem less like Halloween and more happyish ![:)](./images/smilies/smile.gif)
I'm going to try the strontium fire in a few days. I soaked some pine cones in a saturated solution of strontium chloride and I'm going to toss a few
in a fire.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I bought 20L of methanol otc from a place that does specialist fuels and oils for performance cars. It is also sold for remote control planes. Shop
around hobby stores.
[edit] located in oz.
[Edited on 19-12-2017 by j_sum1]
|
|
AngelEyes
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 187
Registered: 24-1-2003
Location: South of England
Member Is Offline
Mood: Better than it used to be.
|
|
Biodiesel suppliers is where I buy my methanol.
Also, lithium salts burn red too...can you source lithium chloride? Burns a decent red in methanol. I never had much success with strontium.
\'Silk and satin, leather and lace...black panties with an Angel\'s face\'
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3630
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
To get a nice green flame I used Boric Acid and Methanol,
ethanol (methylated spirits) gives a slight yellow tinge to the flame, as does borax (sodium borate).
Also, if using a wick, it must be clean and trimmed to avoid yellow from carbon soot.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
Even the smallest trace of sodium will overwhelm the green tint with yellow. You really should look harder for boric acid. It's often sold as a
low-toxicity anti-cockroach powder. Check the labels, and look for "100% boric acid".
To get the green color, you need to form borate esters, so you need to remove water somehow. Sulfuric acid is one option, but it'll interfere with
the flame in many cases. So try mixing methylated spirits (denatured alcohol) with boric acid and silica gel, then shaking the mixture periodically.
You can get silica gel by cutting open desiccant packs, and some places sell it as well.
If propylene glycol is easy to get, I've had very good luck mixing that with boric acid, although you have to give it some time to form the borate
ester (about a day or so). It burns with an emerald-green flame, and burns more slowly than methanol does.
[Edited on 12/19/17 by Melgar]
The first step in the process of learning something is admitting that you don't know it already.
I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
|
|
Rhodanide
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 348
Registered: 23-7-2015
Location: The 80s
Member Is Offline
Mood: That retro aesthetic
|
|
Quote: Originally posted by goldensquid2000 ![](images/xpblue/lastpost.gif) | First up, I'm just going to put it out there that this is my first post, so soz in advance if I accidentally post in the wrong thread or something
else like that (:
So, I want to make some nice green flames for the family in conjunction with the red strontium flames I'm making (it's the whole "red and green"
Christmas theme). I've got some borax (aka sodium borate or disodium tetraborate Na2B4O7) that allegedly burns green when prepared properly.
According to my knowledge, the sodium cation in borax causes borax to normally burn yellow when dissolved in water. However, upon adding methanol
(CH3OH), trimethyl borate is formed. The prescence of the borate ion turns the flame green during combustion.
Now, I'm having difficulty finding methanol, but I have frequently found methylated spirits being sold in my area. According to what I've searched up,
methylated spirits are virtually just 10% methanol and 90% ethanol, so this stuff contains two types of alkanols that should react with borax. My
question here is, can methylated spirits be substituted with methanol in mixing borax to produce green flames, or does the ethanol somehow not work?
|
Methanol is easily available in not only vehicle parts stores such as Napa and/or VIP, as well as being readily available at most gas
stations!
It's in a bright yellow plastic bottle, usually located near to other vehicle fluids. It's small, and has a base about 3 or so inches wide, with a
thin tapering neck about 2 centimeters wide, of a circular shape. It goes under the brand name "Heet" gas line antifreeze and water remover. It's
usually right next to an identical RED bottle, which for this purpose is NOT what you want. The red bottle contains ISOPROPANOL, and the yellow one
contains METHANOL, which is the one you want. Hope this helps, I'll also slide in a picture of the bottle below, if that helps you more. (NOTE: Since
I now see that you're in Australia, availability for you may be different. Regardless, check both hardware stores, auto part stores, and maybe even
gas stations.)
Right! Now the Boric acid. You don't want to use the Borax, as the Sodium contained in it will overwhelm the Boron's green color with it's bright
yellow hue. You need Boric acid! You can find it most reliably in any hardware store which carries it. You may need to do some research, as I guess
you're in Australia and I'm in the US, so your stores and the availability of products are likely different. It's most commonly sold as a cockroach
killer, and comes in the form of a fine white powder. Container types may vary where you live, but they should all say the same thing. Check it's
ingredients first, of course! I've left an example picture of the kind that they sell near me.
Best of luck, and Happy Holidays!
-R/T
![download.jpg - 9kB download.jpg - 9kB](http://www.sciencemadness.org/talk/files.php?pid=500944&aid=63379)
![41x1Gl9Y-VL._SL500_AC_SS350_.jpg - 17kB](http://www.sciencemadness.org/talk/files.php?pid=500944&aid=63382)
[Edited on 19-12-2017 by Tetra]
[Edited on 19-12-2017 by Tetra]
|
|
Chemetix
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline
Mood: Wavering between lucidity and madness
|
|
Look for water softener in pool shops, check the labels but you will find some that are 100% boric acid. I'm in Aus btw.
|
|