devilunix
Harmless
Posts: 10
Registered: 2-4-2017
Member Is Offline
Mood: No Mood
|
|
Filter issue recycling pet
hello folks.im trying to recycle pet as dioctyl terephthalate .Reacting with octanol.After reaction i see white slime in product.It makes filter
hard.Cant pass product through filter.i think slime is monomer of pet unreacted.Any idea to get rid of ?
|
|
gdflp
|
Thread Moved 24-8-2017 at 10:07 |
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
First off, try and all-caps acronyms, especially if they're subject to multiple interpretations. I came in here wondering if you got cut off writing
"petroleum ether" or something.
Second, it breaks down into oligomers first, before gradually breaking down further. It sounds like that's what you have. You'd probably have to use
a large excess of octanol to drive the reaction towards dioctyl terephthalate.
The first step in the process of learning something is admitting that you don't know it already.
I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1848
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
@ devilunix; most of us can't mind read and my crystal balls are getting a bit mirky these days so could you please give us a bit more detail. For
instance did you isolate the terephthalic acid first? Under what conditions did you try to esterify it? Are we talking n- , iso- or some other octanol
isomer.
Sodium bicarbonate solution can be used to remove the un-reacted terephthalic acid and any mono-ester. Its possible that any free mono-ester acts as
an emulsifying agent but turning it into a salt may not cure this.
|
|
devilunix
Harmless
Posts: 10
Registered: 2-4-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) | @ devilunix; most of us can't mind read and my crystal balls are getting a bit mirky these days so could you please give us a bit more detail. For
instance did you isolate the terephthalic acid first? Under what conditions did you try to esterify it? Are we talking n- , iso- or some other octanol
isomer.
Sodium bicarbonate solution can be used to remove the un-reacted terephthalic acid and any mono-ester. Its possible that any free mono-ester acts as
an emulsifying agent but turning it into a salt may not cure this. |
sorry.i use isooctanol.i dont isolate terephtalic acid.just put pet and isooctanol into reactor.heat it up.use titan catalyst.max 1.4bar 225 celcius
degree temperature.
[Edited on 24-8-2017 by devilunix]
|
|
devilunix
Harmless
Posts: 10
Registered: 2-4-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Melgar ![](images/xpblue/lastpost.gif) | First off, try and all-caps acronyms, especially if they're subject to multiple interpretations. I came in here wondering if you got cut off writing
"petroleum ether" or something.
Second, it breaks down into oligomers first, before gradually breaking down further. It sounds like that's what you have. You'd probably have to use
a large excess of octanol to drive the reaction towards dioctyl terephthalate. |
i use 1:3 pet/alcohol weight
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
You're dissolving your pets in alcohol? Oh, right... PET.
That's really only a 50% excess. Try with like a 200% excess on a small scale and see if it improves? I'm assuming it can be recycled anyway, no?
The first step in the process of learning something is admitting that you don't know it already.
I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1848
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
Do you have a reference to this "titan" catalyst and indeed to the whole process? I have only seen references to direct alcoholisis with low weight
methanol and ethanol they didn't mention C8 alcohols.
|
|