Hello. I got interested in WFNA, as it has very little info on wikipedia. My current guess on its prep is a nitric acid synthesis without water, and
maybe bubbled with air afterward? Or added a little bit of urea? Can someone clarify a little bit? Thanks
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
There are YT vids on the synthesis. Not dissimilar from making azeotropic NA. Simply distil from sulfuric acid and a dry nitrate.
Red fuming nitric acid occurs is you get any evolution of nitrogen oxides. Then you need to redistil.
But really, why? 68% is suitable for nearly everything. And WFNA is painful to store.
Make in small volumes as you need it.
|
|
Booze
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 26-2-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | There are YT vids on the synthesis. Not dissimilar from making azeotropic NA. Simply distil from sulfuric acid and a dry nitrate.
Red fuming nitric acid occurs is you get any evolution of nitrogen oxides. Then you need to redistil.
But really, why? 68% is suitable for nearly everything. And WFNA is painful to store.
Make in small volumes as you need it. |
I wasn't going to make much, or keep it for very long.
Possible RDX synth.
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
Before I could get 68% nitric acid OTC, my nitric acid was always WFNA, because I had to make it myself. It's actually not that bad, in my opinion.
I just stored it in a dark brown polyethylene bottle and never had a problem. Basically, if you vacuum-distill sulfuric acid and 68% nitric acid, or
sulfuric acid and a nitrate salt, you get WFNA. If you distill it without a vacuum, it's less white and more red. Of course, the vapors will destroy
just about anything that you'd use to pull a vacuum except an aspirator, so keep that in mind.
|
|
Praxichys
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline
Mood: Coprecipitated
|
|
I usually distilled KNO3 and H2SO4 without a vacuum to get RFNA and then used a fishtank air pump to blow dry air through it to kick out the
NOx until water clear.
|
|
Booze
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 26-2-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Praxichys ![](images/xpblue/lastpost.gif) | I usually distilled KNO3 and H2SO4 without a vacuum to get RFNA and then used a fishtank air pump to blow dry air through it to kick out the
NOx until water clear. |
I have a pump, but really don't want to risk destroying it. I will do that.
|
|
ave369
Eastern European Lady of Mad Science
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 596
Registered: 8-7-2015
Location: No Location
Member Is Offline
Mood: No Mood
|
|
I've made WFNA successfully using battery acid boiled down to 90%, fertilizer grade potassium nitrate and a retort. Density measurements showed the
concentration to be 95%. The trick is not to overheat the distilling flask, or you'll get RFNA instead.
Smells like ammonia....
|
|
CuReUS
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 928
Registered: 9-9-2014
Member Is Offline
Mood: No Mood
|
|
While we are on the topic of W/RFNA,could someone answer these questions please -http://www.sciencemadness.org/talk/viewthread.php?tid=71219#...
|
|
akmetal
Harmless
Posts: 42
Registered: 20-11-2023
Member Is Offline
|
|
Quote: Originally posted by Booze ![](images/xpblue/lastpost.gif) | Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | There are YT vids on the synthesis. Not dissimilar from making azeotropic NA. Simply distil from sulfuric acid and a dry nitrate.
Red fuming nitric acid occurs is you get any evolution of nitrogen oxides. Then you need to redistil.
But really, why? 68% is suitable for nearly everything. And WFNA is painful to store.
Make in small volumes as you need it. |
I wasn't going to make much, or keep it for very long.
Possible RDX synth. |
Very easy to just get an ATF permit, and if you use it the same day you dont have to have a magazine, even if you have to build a magazine its not
that big of a deal unless you live in a highly urban area.
|
|
thermochromic
Harmless
Posts: 11
Registered: 17-1-2018
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by akmetal ![](images/xpblue/lastpost.gif) | Quote: Originally posted by Booze ![](images/xpblue/lastpost.gif) | Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | There are YT vids on the synthesis. Not dissimilar from making azeotropic NA. Simply distil from sulfuric acid and a dry nitrate.
Red fuming nitric acid occurs is you get any evolution of nitrogen oxides. Then you need to redistil.
But really, why? 68% is suitable for nearly everything. And WFNA is painful to store.
Make in small volumes as you need it. |
I wasn't going to make much, or keep it for very long.
Possible RDX synth. |
Very easy to just get an ATF permit, and if you use it the same day you dont have to have a magazine, even if you have to build a magazine its not
that big of a deal unless you live in a highly urban area. |
Someone can correct me if I am wrong but I am pretty sure you do not need any permit from the AFT to simply synth rdx or other energetic (minus a few
outlawed by name like TATP). Permitting is required for transportation, storage, or if you are making a destructive device. Is far is the “ if you
use it on the same day” statement, I think you are thinking of ffl 07/SOT requirements for serializing and logging destructive devices. Perhaps
there is a similar requirement for record keeping of explosives but like I said, if you are making some, not transporting, and using experimentally
the same day on your own property, no licensing is needed, federally at least
[Edited on 24-12-2023 by thermochromic]
|
|
Rainwater
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 859
Registered: 22-12-2021
Member Is Offline
Mood: indisposition to activity
|
|
In the US, federal level, your correct.
But every state has different restrictions, and every county, more restrictions.
There is not a one size fits all answer here.
Best to ask your local authorities.
Most will be understanding, some will think your a nut job.
Mine wanted to see me workspace and lab logs.
Since moving into a more populated area, i was granted permission for quantities less than 0.1g.
and local noise/firework restrictions apply.
[Edited on 24-12-2023 by Rainwater]
"You can't do that" - challenge accepted
|
|