Does anyone know a test that would distinguish one from the other?
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
An easy way to tell them apart would be by density (if you have enough material). Beryllium oxide is 3.01 g/mL and aluminum oxide is 3.95 g/mL.
|
|
Eric Slighton
Harmless
Posts: 6
Registered: 23-5-2015
Member Is Offline
Mood: No Mood
|
|
Hmm... It is in an assembly & hard to take out.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I assume you are looking at gemstones -- essentially looking at the difference between beryl/emerald/aquamarine and rubies
A hardness test might help. But if that is your context I would consider getting it appraised by an expert. The crystal structures are different
(trigonal vs hexagonal). Refractive index and birefringent properties also differ. But I doubt there is anything really simple that you could do to
tell them apart.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Topaz should be harder than beryllium oxide, but less hard than alumina.
Why do you want to know? Is it an electrical insulator?
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | I assume you are looking at gemstones -- essentially looking at the difference between beryl/emerald/aquamarine and rubies. |
Beryl isn't beryllium oxide. It's a beryllium aluminum silicate (as are emerald and aquamarine).
Topaz is also different. I don't think the OP was asking about gemstones (since in that case the post would have specifically mentioned the gemstone
names).
[Edited on 10-30-2016 by Metacelsus]
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Metacelsus ![](images/xpblue/lastpost.gif) | Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | I assume you are looking at gemstones -- essentially looking at the difference between beryl/emerald/aquamarine and rubies. |
Beryl isn't beryllium oxide. It's a beryllium aluminum silicate (as are emerald and aquamarine).
Topaz is also different. I don't think the OP was asking about gemstones (since in that case the post would have specifically mentioned the gemstone
names).
[Edited on 10-30-2016 by Metacelsus] |
Topaz is one of the reference materials on the Moh's scale of hardness. It really doesn't matter in this context if it's made from eye of newt.
|
|
zed
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Huh? You have to give us more information. I had a buddy that sometimes used Beryllium Oxide, in prototype electronics applications. Mixed it with
grease, that he applied at Power Transistor/Heatsink junctions.
In later years, this caused me stop everything, and thoroughly wash my hands every time I encountered white grease inside an electronics devise.
Beryllium Oxide can mess you up. Skin exposure too.
https://en.wikipedia.org/wiki/Beryllium_oxide
https://en.wikipedia.org/wiki/Berylliosis
[Edited on 30-10-2016 by zed]
[Edited on 30-10-2016 by zed]
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Quote: Originally posted by Metacelsus ![](images/xpblue/lastpost.gif) | Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | I assume you are looking at gemstones -- essentially looking at the difference between beryl/emerald/aquamarine and rubies. |
Beryl isn't beryllium oxide. It's a beryllium aluminum silicate (as are emerald and aquamarine).
Topaz is also different. I don't think the OP was asking about gemstones (since in that case the post would have specifically mentioned the gemstone
names).
[Edited on 10-30-2016 by Metacelsus] |
Good point. Well spotted.
I reacted to the comment that it was attached to something. So this makes me wonder what the application is. I am struggling to conceive of a
situation where the two could be confused.
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Most likely that SeƱor Eric is taking a microwave oven apart and is worried about the beryllium oxide used in the making of the magnetron.
It would help if the OP could be more specific about what they are doings/wantings knowings of.
[Edited on 30-10-2016 by aga]
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
There are no significant amounts of beryllium oxide in domestic microwave oven magnetrons.
There is no reason why there would be. These days if there was the oven would probably require a health warning along with its magnetron and the sale
of such ovens would be illegal in California and probably the EU as well LOL.
|
|