Platinum Catalyst Mount
Recently I obtained some platinum wire to use as a catalyst. My planned reaction is making NO2 from ammonia and oxygen and then bubble it through
water or hydrogen peroxide to make nitric acid. This reaction causes the platinum to heat up a lot. Obviously I don't want it to contact any glassware
because the glass may break or melt. What is the best way to position the wire for the best reaction and safest process?
|
|
NitratedKittens
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 131
Registered: 13-4-2015
Location: In the basket with all the other kittens
Member Is Offline
Mood: Carbonated
|
|
Maybe make a reaction vessel out of a steel can to house the platinum wire.
[Edited on 2-12-2016 by NitratedKittens]
Basket of kittens for you ........BOOM
|
|
Chlorine
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 56
Registered: 26-11-2016
Location: Maine, USA
Member Is Offline
Mood: Brominated
|
|
Attach the Platinum wire to a lab stand and position it so it hangs in the middle of the beaker/flask.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Toast ?
http://www.sciencemadness.org/talk/viewthread.php?tid=70570
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Chemetix
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline
Mood: Wavering between lucidity and madness
|
|
Quartz tube- from an old heater
|
|