Neme
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 86
Registered: 28-5-2016
Location: Czech republic
Member Is Offline
Mood: No Mood
|
|
Best way to preserve crystal
As it is written in the tittle, I'm looking for new method to preserve crystals.
I've tried so far:
water glass --> reacted with crystal compound --> failure
spray transparent paint --> not 100% efficient, got blank spaces
nail polish --> heterogenous layer which is not looking good
I need it mainly for mine chrome alum crystals like this one:
|
|
yobbo II
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
Something like this?
http://www.ebay.co.uk/itm/OptiCast-100-Water-Clear-Polyureth...
There are cheaper kits if you look
|
|
Neme
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 86
Registered: 28-5-2016
Location: Czech republic
Member Is Offline
Mood: No Mood
|
|
I'd rather keep the shape of the crystal as it is, not a cube with crystal inside, but thank you for tip
|
|
Dmishin
Harmless
Posts: 32
Registered: 5-10-2015
Member Is Offline
Mood: No Mood
|
|
You can grow a layer of more stable, transparent alum over it. I did it with ferric alum (that is also unstable and turns brown in a day), it lives
for a year already.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
I found a solution of "Velpon" glue (a brand) in acetone to be effective in preserving pyritized fossils. It might work well for your application as
well.
A publication from our National Cultural Heritage Agency (very knowledgable in the area of preserving a wide range of historically important objects)
suggests that wood lacquers (for instance lacquers used for wooden boats) and the above mentioned mixture of "velpon" glue in acetone would also be
among the approaches they would consider.
I have no idea (and would be interested to find out) if "Velpon" glue is available in other countries at all, and what is composed of (should the
manufacturer ever go out of business).
[Edited on 25-10-2016 by phlogiston]
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Neme
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 86
Registered: 28-5-2016
Location: Czech republic
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Dmishin ![](images/xpblue/lastpost.gif) | You can grow a layer of more stable, transparent alum over it. I did it with ferric alum (that is also unstable and turns brown in a day), it lives
for a year already. |
That's actually pretty good idea, did you use potassium aluminium alum or ammonium potassium alum or different one?
Quote: Originally posted by phlogiston ![](images/xpblue/lastpost.gif) | I found a solution of "Velpon" glue (a brand) in acetone to be effective in preserving pyritized fossils. It might work well for your application as
well.
A publication from our National Cultural Heritage Agency (very knowledgable in the area of preserving a wide range of historically important objects)
suggests that wood lacquers (for instance lacquers used for wooden boats) and the above mentioned mixture of "velpon" glue in acetone would also be
among the approaches they would consider.
I have no idea (and would be interested to find out) if "Velpon" glue is available in other countries at all, and what is composed of (should the
manufacturer ever go out of business).
[Edited on 25-10-2016 by phlogiston] |
I've never seen it in shop but I can get it from ebay, I'm gonna look at it.
|
|
Dmishin
Harmless
Posts: 32
Registered: 5-10-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Neme ![](images/xpblue/lastpost.gif) |
That's actually pretty good idea, did you use potassium aluminium alum or ammonium potassium alum or different one?
|
I used ammonium aluminium alum, to have common ion with ferric alum. By the way, covering ferric alum was not easy because of very large difference in
solubility; I ended up making several layers, gradually replacing Fe(3+) with Al(3+). With chrome alum, such complications are not needed.
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Another interesting material is Paraloid B72. It is a polymer that is used to conserve all kinds of objects, including fossils and crystals. It is not
expensive and can be dissolved in several different solvents, including acetone and ethyl acetate.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Texium
|
Thread Moved 12-11-2016 at 20:50 |
Neme
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 86
Registered: 28-5-2016
Location: Czech republic
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by phlogiston ![](images/xpblue/lastpost.gif) | Another interesting material is Paraloid B72. It is a polymer that is used to conserve all kinds of objects, including fossils and crystals. It is not
expensive and can be dissolved in several different solvents, including acetone and ethyl acetate. |
I've checked it and it looks like a very good way, but it's really expensive...
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Since you probably do not need to re-use the crystal ingredients
and want to allow others to handle it - safely
would a clear casting resin be suitable ?
e.g. http://www.ebay.co.uk/itm/Casting-King-SUPACLEAR-water-clear...
(choosing the mould as small as possible saves resin)
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Dwarvensilver
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 52
Registered: 8-6-2016
Member Is Offline
Mood: Constantly Chemically Amazed
|
|
HI All,
I too have been trying to preserve crystals from absorbing or losing water but not much success yet and have tried the list that Neme has posted
above. I tried pouring a water clear bar top type resin over Copper sulfate crystals and the darn things are resin phobic, it just ran slowly off
leaving a few clear islands of resin. Even when trying to pour several layers in a crystallizing dish ultimately worked but it was not real pretty and
some areas of the crystal had what seemed like a really thin layer of air at the crystal interface that was not there before curing which cut down on
the viewing pleasure somewhat. Don't know if it will happen with different resin, chemical combinations? Maybe coat with spray or nail polish first?
Encapsulation may work but the only method I have seen so far is to make an open sided box out of plexi, lexan or some such then after curing cut
lexan off and polish all the sides. The time involved is substantial tho.
[Edited on 2016-11-13 by Dwarvensilver]
This looks promising
https://www.youtube.com/watch?v=-daK0wBEA3E
I will have to try this, I went to the mold website and they have a couple of nice molds, square and round.
http://alamould.com/product/cube-mold-home-decor/
[Edited on 2016-11-13 by Dwarvensilver]
There is nothing more useless than doing well that which need not be done at all.
|
|