How to protect concrete surfaces from corrosive attack of CAN ?
How to protect concrete surfaces from corrosive attack of CAN fertilizer (calcium ammonium nitrate)?
When CAN absorbs moisture from atmosphere, it becomes extremely corrosive for concrete.
Can anyone answer me ?
Thanks!!
My mail: celia1095@qq.com )
|
|
celia1095
Harmless
Posts: 5
Registered: 11-4-2016
Member Is Offline
Mood: No Mood
|
|
What's the difference of CAN 26% and CAN 15.5% used in fertilizer ?
What's the difference of CAN 26% and CAN 15.5% used in fertilizer ?
CAN means Calcium Ammonium Nitrate.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
At the risk of sounding simplistic, keep it off the concrete.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
10.5%
Joking aside, if you are after information on products available in your area then your best solution is to look at the label or look up the msds.
Most of us are msds junkies.
This kind of question belongs in the Beginnings section. Anything without a reference does. And Organic Chemistry is for (surprise) organic chemistry.
Welcome to SM. Stick around and enjoy the wealth of information here. Do read the faq and get used to this board's culture.
|
|
hissingnoise
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
In keeping with the simplistic theme, you could, possibly, care to check out the answer already given in your identical first post!
|
|
hissingnoise
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Quote: | What's the difference of CAN 26% and CAN 15.5% used in fertilizer ? |
C.A.N possibly contains 15.5% nitric-N (rapid absorption) and 10.5 ammoniacal-N . . . ?
|
|
Texium
|
Thread Moved 19-4-2016 at 06:03 |
Texium
|
Threads Merged 19-4-2016 at 06:04 |
celia1095
Harmless
Posts: 5
Registered: 11-4-2016
Member Is Offline
Mood: No Mood
|
|
Thanks so much
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Actually, a more interesting and not an answer for the Beginnings section is why/how is the concrete corroding? To answer, a lot more info like what
is type of concrete? Do different fertilizers behave similarly with this concrete? Soil pH, rain water pH, moisture conditions, presence of iron
salts,... some possible factors.
Understanding the causality may present an answer to how to avoid/stop further corrosion both visible above ground and hidden underground.
I suspect galvanic corrosion from an Fe presence To verify, place a small amount of sea salt in one of the corroding areas. If significant
acceleration, a confirmation of either electrochemical reaction or an increase in the "activity coefficient" of an acid/base attack. If the pH in the
area is low, add a base with more sea salt. If still corroding, than likely galvanic ( and there may be related solutions)..
|
|