raghotham
Harmless
Posts: 1
Registered: 4-4-2016
Member Is Offline
Mood: No Mood
|
|
SAPARATE SILVER FROM TIN SOLDER
dear sir
i have very huge qty of solder which is used for soldering the electronics
in witch it contains 96% tin 0.76 % copper and silver 2.87%
i need to separate the silver and copper form this alloy
please suggest me how to process
thanking you
raghotham
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Before you start with this project, consider that is may be more economical, easier and better for the environment if you just sell the stuff to a
metal recycling company that have experience in this, can handle large quantities and benefit from the economy of scale.
Then just buy the silver and copper you need.
The silver content is so low, it is likely that you'll spend more on chemicals and other consumables than the silver is worth.
[Edited on 5-4-2016 by phlogiston]
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Send it to the tin refiner?
Otherwise plate the tin out?
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
DFliyerz
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 241
Registered: 22-12-2014
Member Is Offline
Mood: No Mood
|
|
Dissolve the tin with hydrochloric acid, which you can then electroplate out to recover. Dissolve the residue that is insoluble in hydrochloric acid
with nitric acid, and add copper wire to precipitate out the silver metal.
|
|
Texium
|