Getting powder Al from electrolyisis
Hello everyone,
I have recently bought some aluminum sulfate do try to get some aluminum powder (or little particles) from it. The problem is that it's not possible
to make aquous electrolysis with it, can anyone help me please?
Thanks
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Buy some Al powder.
Or make your own. I purchased a second-hand food processor and ground away at some aluminium foil. It takes some time but it works.Some fine sieves
help to grade your product. I have heard that adding liquid while grinding helps a lot. But I have not tried that.
|
|
Dark Alchemist
Harmless
Posts: 38
Registered: 14-11-2015
Location: Behind you. No really look!!!
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by eanardi ![](images/xpblue/lastpost.gif) | Hello everyone,
I have recently bought some aluminum sulfate do try to get some aluminum powder (or little particles) from it. The problem is that it's not possible
to make aquous electrolysis with it, can anyone help me please?
Thanks |
If you want good quality Al powder I would recommend investing in a cheap rock tumbler some lead sinkers and a coffee grinder as he said.
Is it for lab use or pyro use? if for lab use small marbles instead of sinkers as the sinkers leave behind some lead dust that can contaminate your Al
when used as tumbling media.
PS YouTube is your friend.
If your not on a government watch list by now you should be ashamed of yourself.
|
|
Dark Alchemist
Harmless
Posts: 38
Registered: 14-11-2015
Location: Behind you. No really look!!!
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by eanardi ![](images/xpblue/lastpost.gif) | Hello everyone,
I have recently bought some aluminum sulfate do try to get some aluminum powder (or little particles) from it. The problem is that it's not possible
to make aquous electrolysis with it, can anyone help me please?
Thanks |
If you want good quality Al powder I would recommend investing in a cheap rock tumbler some lead sinkers and a coffee grinder as he said.
Is it for lab use or pyro use? if for lab use small marbles instead of sinkers as the sinkers leave behind some lead dust that can contaminate your Al
when used as tumbling media.
PS YouTube is your friend.
If your not on a government watch list by now you should be ashamed of yourself.
|
|
Chemist_Cup_Noodles
Harmless
Posts: 46
Registered: 27-5-2015
Location: Northern VA
Member Is Offline
Mood: Anticipative
|
|
Hmm, it could be possible to do a replacement reaction with it instead. If you have some magnesium metal, use some filings of that. The reaction
should be 3Mg2+(s) + Al2(SO4)3(aq)-->2Al3+(s) + 3MgSO4(aq). Just prepare maybe a 1M solution of aluminum sulfate then add 72 grams of magnesium
filings bit by bit, over gentle heat initially. You'd get a good solution of epsoms salts too, which is nice. You could probably filter out an
aluminum slurry from this. If I'm wrong about this someone please correct me.
|
|
Amos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
I'm not sure if magnesium is even reactive enough to displace aluminium, but magnesium powder is often more expensive than aluminium powder, plus
aluminium powder being generated in solution would likely immediately convert the aluminium being formed to oxides and hydroxides.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Mg is more expensive, more difficult to obtain and more reactive than Al. So, in principle you cold use it. But you would still have to get around
the hydroxide issue. I wouldn't bother with that route for a second.
Where are you located, earnadi? I know a supplier in Aus that can do 1kg of Al powder for twenty bucks. PM me if that is useful for you.
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1701
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
You cannot precipitate aluminum metal in water, it's simply too reactive. The only route to powder is to start with metal and grind/mill it down.
We're not banging rocks together here. We know how to put a man back together.
|
|
eanardi
Harmless
Posts: 10
Registered: 20-11-2015
Location: Inside a buckyball -BR-
Member Is Offline
Mood: No Mood
|
|
That'd be useful if I didn't live in Brazil but thanks for the tip
All the information here was very useful, thanks everyone!
|
|
Sakomekieh
Harmless
Posts: 4
Registered: 25-9-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by eanardi ![](images/xpblue/lastpost.gif) | That'd be useful if I didn't live in Brazil but thanks for the tip
All the information here was very useful, thanks everyone! |
I live in Brazil, too. You can simply build your own ball mill, it isn't that hard. There is many good videos teaching how to build a ball mill in
youtube, you just need to search it.
|
|
eanardi
Harmless
Posts: 10
Registered: 20-11-2015
Location: Inside a buckyball -BR-
Member Is Offline
Mood: No Mood
|
|
I'll start mine tomorrow. Just bought my motor, if you have one, would you mind sending me a photo of it?
|
|