diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
Liquified gasses in ampoules
Seeking any thoughts on ampouling liquid chlorine. and just for interest, has anyone tried ampoule of LN2. I don't have access to anything colder than
LN2, so maybe I cant do it?
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
How often do we do this diddi? Your questions are similar to mine.
That said, I have read a couple of threads on ampouling. I would be surprised if liquid chlorine hasn't been covered already.
I have seen nice quartz samples of liquid chlorine. I am not sure how much internal pressure is an issue and whether you would get away with regular
glass ampoules. I know there are issues with pressurising a gas in an ampoule.
Woelen posted in one of these threads some ampoules of gaseous Cl2 that he made. His pix are in the Wikipedia entry on Chlorine if I recall
correctly.
My plan is to have a go at ampouling Cl2 gas first. I will then have a go at liquid. I will use dry ice and acetone to get Cl2 down to the required
temperature. Then a separate container without the acetone to hold the temp down while I seal the ampoule. (I really don't want an acetone flare up
while attempting to melt the glass.)
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
I have seen a bit here and there as well, but nice to have any recent updates. at room temp chlorine has vapour pressure of about 10atm, so good glass
should contain it OK. I want to try making an ampoule out of borosilicate test tubes to see what they are like. maybe abject failure, but wont know
until I try. I will use LN2 for my cold bath. no fire problems that way and the vapour above the liquid is useful to provide a temp gradient rather
than in or out of a liquid with no in between.
also considering liquid O2 and Ar.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Sounds like you have access to a few better resources than I do.
Your element collection should be a stunning piece of work when it all comes together.
Let me know how you get on.
Chlorine aside, then next serious ampoule that I do will be bromine. I have a thick walled 10mL graduated pipette where the markings have rubbed off.
I figure that it will be a great-looking sample if I 3/4 fill it with bromine. I got some glassware today and so I will get on to it in the next
spare weekend -- which unfortunately is likely to be a month away still.
(Or maybe the boron project will come first.)
|
|