Author: Subject: agricultural KCl
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 31-3-2013 at 08:17


Use multiple cells in series if you are going to use 30V.
You should be able to do about 7 cells with good results.
View user's profile View All Posts By User
Steve_hi
Hazard to Others
***




Posts: 196
Registered: 4-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 31-3-2013 at 13:38


Should have said variable 0- 30v 0-10A so one cell will be enough.

[img]C:\Users\Steve\Pictures\Power supply.jpg[/img]

Power supply.jpg - 57kB
View user's profile View All Posts By User
plante1999
International Hazard
*****




Posts: 1936
Registered: 27-12-2010
Member Is Offline

Mood: Mad as a hatter

[*] posted on 31-3-2013 at 17:26


then use 3.33 V, and not more than 0.03 amp per square cm area of the graphite anode.



I never asked for this.
View user's profile View All Posts By User