hypochlorite solution with crystals in it
I used sulfuric acid and commercial bleach (basically sodium hypochlorite with undesirables in it) to generate a gas stream that was neutralized by
sodium hydroxide (2.5M). The mass of this solution was recorded and it is quite consistent with conversion of hydroxide to hypochlorite.
The bottle contains small thin crystals now, though. What could this be?
[Edited on 18-10-2012 by Cloner]
|
|
99chemicals
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 174
Registered: 24-3-2012
Location: In the Octet
Member Is Offline
Mood: No Mood
|
|
Which bottle had the crystals? The bottle with the impure bleach or the bottle that you converted NaOH to NaClO.
|
|
Ephesian
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 97
Registered: 14-8-2012
Member Is Offline
Mood: No Mood
|
|
what bottle are we talking about here...
[Edited on 18-10-2012 by Ephesian]
|
|
tetrahedron
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 210
Registered: 28-9-2012
Member Is Offline
Mood: No Mood
|
|
sodium chloride was also generated in the conversion.
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Yeah, but he said thin crystals. NaCl is cubic.
|
|
tetrahedron
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 210
Registered: 28-9-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Cloner ![](images/xpblue/lastpost.gif) |
The mass of this solution was recorded and it is quite consistent with conversion of hydroxide to hypochlorite.[Edited on 18-10-2012 by Cloner]
|
how did you measure this?
how about the purity of your NaOH? maybe it was tainted with carbonate or acetate. if only gas was passed it's unlikely that the crystals are due to
impurities in the H2SO4 or bleach.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
I suspect sodium sulfate decahydrate. Remove some crystals, do they turn white and powdery on drying in air?
Tim
|
|
Cloner
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 150
Registered: 7-12-2004
Member Is Offline
Mood: apocalyptic
|
|
The impure bleach and sulfuric acid were used to generate a gas stream, the gas was led through hydroxide solution. The resulting solution of
hypochlorite contained the crystals.
Mass was measured of the hydroxide solution and the sodium hydroxide itself. The mass of the sodium hydroxide was 10,04 g, the mass increase was 8,7 g
after the reaction.
edit: the crystals are very insoluble in water. They also produce a rainbow effect. Prismatic form then?
[Edited on 19-10-2012 by Cloner]
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1378
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
It almost sounds like you took KOH instead of NaOH.
Then the crystals would be KClO3, which fit your description well. prismatic, thin and only moderately soluble. KClO3 is well known to form when Cl2
is bubbled through a KOH solution, especially when warm.
crush a few up, mix with sugar 50:50 and try to see if it will burn.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Cloner
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 150
Registered: 7-12-2004
Member Is Offline
Mood: apocalyptic
|
|
You are correct.
To test it out, I added a little KOH. A few more crystals were formed. The NaOH I used will undoubtedly contain minute amounts of potassium impurity.
|
|