Nitrating paper
It is something I really want to know how to do, and cant find out how?(I SWEAR I GOOGLED) I am guessing I want to add KNO3 or NH4NO3 to some mixture
of sulfuric, nitric, or phosphoric acid, then set the paper in and wait. BUT I have learned guessing should be left outside the lab. So basically if
anyone can provide me with a simple method, or 2, or just some information that will help me, it would be much appreciated. I WANT FLASH PAPER!!!!
Thanks
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Obviously you did not look very hard, if you can find someone with access to JCE then there is a good procedure here;
http://jchemed.chem.wisc.edu/journal/Issues/1995/Dec/abs1133...
Apart from that it is widely available online from conjuring shops.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Sam Barro gives a method of preparation;
http://www.powerlabs.org/chemlabs/nitrocellulose.htm
As well as that an experiment which I do as a demo is to spear a ping pong ball on a wooden skewer. This is then ignited by touching the ping pong
ball to the flame of a gas torch at a safe distance. Ping pong balls are made of nitrocellulose and it ignites in a fairly spectacular manner
[Edited on 5-8-2008 by ScienceSquirrel]
|
|
franklyn
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline
Mood: No Mood
|
|
Anytime someone says " I can't find it on google " I wince, thinking to myself
oh no is this being censored, but I have as yet to find this to be the case.
I debated with myself whether to answer since it appears you could not find
your own ass with both hands if I drew you a diagram and took you there by
the wrist. Not confidence inspiring. There is even an entry in wikipedia on this!
Enter these search terms as shown here into google for more information
nitrocellulose "flash paper" magician
What I found
1. You can buy it in any magic store
http://www.hfmgroup.com/professionalsupplies/flashguns.html
2. If the above is not an option
http://collectables.shop.ebay.co.uk/items/Fantasy-Myth-Magic...
3. If you really want to roll your own
http://www.newton.dep.anl.gov/askasci/chem99/chem99569.htm
MSDS - http://www.starmgc.com/MSDSpaper.html
This is not a joke/novelty, it is a pyrotechnic. Beware breathing
fumes from your acid blend, do it outside and stand upwind to the dish.
P.S.
I have not done the following, but I understand that soaking paper in a hot
saturated solution of Potassium chlorate then letting this dry serves much the
same purpose.
.
|
|
sparkgap
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline
Mood: chaotropic
|
|
Well...
If you want a look...
sparky (~_~)
Attachment: nitropaper.pdf (1.4MB) This file has been downloaded 1540 times
"What's UTFSE? I keep hearing about it, but I can't be arsed to search for the answer..."
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
In case you have difficulties finding nitric acid, the book "Caveman Chemistry" describes the nitration of cotton using a paste made with 15g of H2SO4
and 10 grams of potasium (or sodium) nitrate. The Idea is simple: HNO3 gets generated "in situ".
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
If you want a few sheets for demo expts then I would suggest buying it.
Nitrating paper is a lot of trouble on a small scale and that is ignoring the fire risk.
I do chemical demonstrations and the fire risks are always uppermost in my mind.
Setting fire to the audience is not a good idea!
|
|
PyroRA
Harmless
Posts: 18
Registered: 23-6-2008
Member Is Offline
Mood: No Mood
|
|
Thank you guys so much for all the info.
Now this is NOT a professional thing, I just really want to make some, It seems so cool and interesting me, so I don't have nitric acid and
making/obtaining it would be a whole different story, but I can do without by adding KNO3 into the idea, so heres my next question, I am too lazy to
search for, Where can I get/how can I make H2SO4. I thought all this could be done with battery acid, that isn't out of my reach, Heh. Also Would
Acrylonitrile gloves be sufficient in case of contact?
Thanks again.
R.A.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Unless you have access to good reagent grade chemicals and the type of equipment detailed in the JCE paper I would just forget about the whole idea of
making it.
Mixtures of battery acid and potassium nitrate just will not work. It will be a nasty mixture that you will have to dilute and dispose of.
Flash paper is extremely flammable. The commercial material is supplied wet and the people who use it dry it off carefully before use.
If you want to experience the effects of burning nitrocellulose, just try my table tennis ball trick. The ball erupts into a sheet of flame.
Many years ago someone decided to ruin some teenagers' table tennis game by burning a hole in the ball with the tip of his lighted cigarette, he was
taken to hospital with severe burns.
Here is a video of a burning table tennis ball;
http://www.metacafe.com/watch/597183/table_tennis_ball_at_fi...
Nitrocellulose is an interesting material but it has to be treated with respect and handled with the appropriate precautions otherwise you may have a
severe and possibly fatal accident.
[Edited on 8-8-2008 by ScienceSquirrel]
|
|