Dear All,
I am doing the fire assaying process - cupellation. But my silver dope recovery rate is low, less than 90%, there must be the silver loss during the cupellation. Any tips I could follow and be careful?
Thanks.
David 6/7
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 7-6-2007 at 10:07


See this thread:

http://www.sciencemadness.org/talk/viewthread.php?tid=6994&a...


It might be helpful.




The single most important condition for a successful synthesis is good mixing - Nicodem