Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Fibers from green Bamboo
kamal
Harmless
*




Posts: 33
Registered: 14-9-2005
Member Is Offline

Mood: always happy

shocked.gif posted on 16-5-2007 at 20:52
Fibers from green Bamboo


Hi friends...!!

Can I get some suggetions from you friends for making (separating) fibers from a bamboo ? It is a cellulosic material & generally being made commercially thro' like rayon making process & also thro' some mechanical process like crusing, grinding, etc....

However, I'm not having details about any of these proceses.

Is it possible to make suluble the fibers in something & then extracting/separating....??

I will be eagerly awaiting your suggetions.....
View user's profile View All Posts By User
DrP
National Hazard
****




Posts: 625
Registered: 28-9-2005
Member Is Offline

Mood: exothermic

[*] posted on 16-5-2007 at 23:17


I would suggest soaking them and grinding somehow. Then maybe leaving them for a while to soak some more at temperature before grinding them to a pulp. Might be usful to boil your mix up to help break it all down. Wood fibres are made this way (high temp and grinding of a mulch) so I guess it should be simular.

I don't know a chemical way. Certain nonylphenolethoxylates are sometimes used to break pulps down over time - I guess they could work for bamboo as well?

What are you going to add them to?



[Edited on by DrP]
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-5-2007 at 01:35


Soaking in water followed by steam explosion is a preferred method, I believe. Bamboo is more difficult than many other fiber plants to process, because of the hard nodes and higher silica contend; not to mention the ecologists and wildlife preservationists who will protest the destruction of the forests and organise boycotts of your company. Industrial hemp is much easier to deal with.

From my bookmarks:


http://www.inbar.int/publication/txt/INBAR_Working_Paper_No4...

http://cat.inist.fr/?aModele=afficheN&cpsidt=1249946

http://cat.inist.fr/?aModele=afficheN&cpsidt=14887044