Freeze / Thaw Extraction
I've got 3 organic substances, with the following melting points:
A: -83c
B: 30c
C: 70c
Fraction 'B' is the compound to be isolated. Both 'B' and 'C' are solvated by 'A' but do not dissolve in each other.
The theory is like this: if the mix is frozen then 'A' can be discarded as a liquid. Then the mix is gently heated above 30c and 'C' solid can be
discarded, leaving 'B'.
Will it work?
[Edited on 27-2-2007 by Baphomet]
\"Who ARE you? You\'re like the drummer from REO Speedwagon - nobody knows who you are\" from \'Employee of the Month\'
|
|
Maya
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 263
Registered: 3-10-2006
Location: Mercury
Member Is Offline
Mood: molten
|
|
Maybe, or maybe not, generally solubility goes down as temperature goes down but not always. Look up differential crystallization techniques. Are your
compounds Organic or Inorganic?
It all depends on the solubility of fractions B & C in fraction A as a function of temerature.
Thats all I can say with certainty about your theoretical problem set w/o further details
\"Prefiero ser yo extranjero en otras patrias, a serlo en la mia\"
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
B is the lowest melting right?
If so, why not fractionally distill under vacuum?
|
|
YT2095
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
since A is -83 then cant you just leave the whole thing at room temp for a while as it BP will be presumably lower than the BP of the other 2.
that just leaves B and C to sort out.
do you Have the BP data on these or just the MP data?
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
Baphomet
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 211
Registered: 19-11-2006
Member Is Offline
Mood: No Mood
|
|
Thanks guys I tried it but 'A' still had the others in solution at -5c
In the absence of dry ice, a frac dist is the way to go