kadriver
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 7-11-2012
Location: United States
Member Is Offline
Mood: Thankful
|
|
Platinum Refining Practice with a Pure Pt Coin Pt2 - VIDEO
Here is the second half of the Pt refining video
https://youtu.be/HbDwaccp50c
kadriver
Youtube channel - sreetips
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Nice video about Platinum Refining.
Please put a more detailed description in your next post here, as not every member has the bandwidth allowance to watch the utoob video just find out
what the post is about.
You really should heed your own warnings !
The fact that you can speak clearly in some parts of the video means that you were not wearing a gas mask - the dust can get you too.
Pt refiners tend to die young, so Nickvc told me, so stay Safe my friend !
|
|
zed
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Sounded like he was doing the whole procedure in a fume hood. Not perfect protection, but pretty good.
Had no idea Platinum Salts were so toxic.
Usta work with 'em on occasion. Never had a problem.
On the other hand, I usta treat pretty much everything I worked with, as if it were highly toxic. Kinda paranoid, actually.
Quite possibly the reason, I have attained this ancient age, without developing the severe cooties, or the advanced heebie-jeebies.
|
|