CuO/Ca(So4)2 for reducing dialkylimines (Ketone + alkylamine)
I just found this, it is a patent for the preparation of a cheap, easy catalyst (read OTC) for the reduction of the imine product of ketones and
alkylimines
US Patent No. 2828343
http://v3.espacenet.com/textdoc?IDX=US2828343&CY=gb&...
[Sorry, I can't work out how to turn this into a hyperlink)
Unfortunately the patent is only rated for reactions occurring at 200C and between 150-1500 psi. (however, so was Platinum dioxide). It would be
interesting to see if this catalyst could be used at lower temp's & pressures?
It consists of a homogenous mixture of CuO + Ca(SO4)2, prepared (according to the patent) by adding CuSO4 to a paste of CaOH and then heating the
mixture to form the CuO (it goes brown apparently).
This would appear to provide a way cheaper (and simpler) alternative to the purchase and preparation of PtO(2), Pd/C, Ra/Ni, etc. and be more
environmentally responsible than Al/Hg. It would certainly make me smile if it were possible to use a cheaper, less pyro-prone catalyst if I fall
asleep and have one of those unfortunate dream sequences.
By the way, if anybody else reads this catalyst, please don't do anything silly with the knowledge contained therein. And for fucks sake, please DO
NOT make what the person patenting it did at example 1 (what the fuck is desoxy-ephedrine anyway?)
|
|
microswitch
Harmless
Posts: 27
Registered: 26-11-2006
Member Is Offline
Mood: No Mood
|
|
Thanks for the interesting patent. I myself have been doing a lot of research for a ketone to amine reduction that doesnt involve Hg or Cyanide. This
looks like a promising candidate with potential applications for the amine reduction.
\"Conspiracies hatched in hell do not have angels as witnesses,\" Hough said.
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Few thoughts on this.
A goodly percentage of patents never really pan out. They work to some degree, but are too low in yield, too tricky to use on an industrial scale,
make too many side products, don't last long enough, and so on.
Copper usually comes in a distant third for hydrogenation reactions, after platinum metals and nickle (and sometimes cobalt). Test runs using some
cheap and readily available compounds that compared this to more conventional options would be interesting.
This should also work using nickel sulfate in place of copper sulfate. You might even try a mixed Cu-Ni version, using nickel alloy coins dissolved in
aerated not-too-strong sulfuric acid.
|
|