Db33
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 206
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
whats better for storing Toluene?
Right now i have a gallon of Toluene that is still in the metal paint can i got it in. My thoughts are to either leave it in there, or put it in a 1
gallon HDPE bottle , or a 1 gallon wine glass bottle. any thoughts?
|
|
PirateDocBrown
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline
Mood: No Mood
|
|
I see no reason to move it.
|
|
Corrosive Joeseph
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 915
Registered: 17-5-2015
Location: The Other Place
Member Is Offline
Mood: Cyclic
|
|
I use a toluene based thinners when I work on vehicles............
If the can is around a long time I notice the thinners turns a dirty rusty colour...............
There are other solvents mixed in there but I would be of the opinion that any where except the can would be good
/CJ
Being well adjusted to a sick society is no measure of one's mental health
|
|
JJay
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
I usually leave solvents in the can until I get a chance to purify them. I figure why put dirty solvents into nice bottles. I don't use toluene that
much, so I probably won't purify an entire gallon of toluene at once, but I have been meaning to prepare 100 mL or so of nice, dry, thiophene-free
toluene for a while now....
|
|
anewsoul
Harmless
Posts: 32
Registered: 26-1-2017
Member Is Offline
Mood: No Mood
|
|
If I could I would put all my toluene in a different container for convenience sake. It is practically impossible to pour some toluene out of those
metal cans without spilling it everywhere.
|
|