Looking for help building my down's cell
I already know all the physics and chemistry behind but I am looking for some advice from people who have actually built them and can offer some
construction tips
Right now I am looking for a suitable heat source, preferably electric and it must get at least 700 C, I am using a NaCL CaCl mixture
EDIT: I searched this site but found few actual building instructions, mostly just more chemical formulas
[Edited on 27-10-2006 by b_d_Dom]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Have you searched this site to see what work may already have been done on this subject?
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I've built one before, see my references to it in the thread entitled "Hot electrochemical sodium". Also, 700*C is way too hot. Your salt will
volatilize. Please research more. I can send you an email if you like...
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
b_d_Dom
Harmless
Posts: 32
Registered: 27-10-2006
Location: Canada
Member Is Offline
Mood: No Mood
|
|
Ya an email would be great! I sent you an U2U with my address.
Also because I am using the 40% NaCl + 60% CaCl2 mix I would need a minimum of 580 C, and 700 C would be preferable so I can build a larger machine.
|
|