will trade 500 grams of >50% In Alloy for analysis of the alloy


I have 9 samples of an Indium alloy that is well over 50% In (probably close to 75%), as well as one sample that I believe to be 99% In. However, I am wondering if someone with access to an AA or an ICP would be willing to trade the analysis of 9 samples of the alloy (turnings), and an analysis of the 99% for Indium content for one of the 500 gram bars (of the alloy). That means you would be getting more than 250 grams of Indium for perhaps an hour or two's worth of work?

Feel free to PM me if interested! Thanks!
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 9-4-2015 at 15:05


Indium Corp. of America?

I have a couple of "mystery ingots" myself.

image.jpg - 26kB

[Edited on 9-4-2015 by Bert]




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
zephler1
Harmless
*




Posts: 41
Registered: 16-11-2013
Member Is Offline

Mood: No Mood

[*] posted on 9-4-2015 at 16:51


Hi Bert,

LOL - "mystery ingots". No, they were a bunch of scraps from a CIGS Solar operation at one point. I've had them for 10+ years from my days as an electronics scrap cowboy and recently with the price of indium going up, I've melted them into 500 gram ingots using the old "muffin ingot" tray. My data sheet with them is missing a few values, but I would like to get a number from this decade on these new tasty looking metal snacks.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 9-4-2015 at 17:27


z1:

What's supposed to be the remainder of the alloy?

[Edited on 10-4-2015 by blogfast25]




View user's profile View All Posts By User
zephler1
Harmless
*




Posts: 41
Registered: 16-11-2013
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2015 at 01:08


50 -70% Indium / 40 - 20% Gallium / 10% Copper / <1% Selenium
View user's profile View All Posts By User
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 10-4-2015 at 12:35


How accurate do you need the analysis? I use a handheld XRF spectrometer (Niton XLp) at work daily and could easily check out your alloy. However it doesn't provide more than one decimal point (I think? It may be two, when I think of it) of accuracy and I'm not sure how accurate it actually is.



This just in: 95,5 % of the world population lives outside the USA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User
smaerd
International Hazard
*****




Posts: 1262
Registered: 23-1-2010
Member Is Offline

Mood: hmm...

[*] posted on 10-4-2015 at 18:23


I have access to an AA but only for a few more weeks and I don't think we have an In tube :(. Maybe in a few months though.



View user's profile View All Posts By User
cmos6667
Hazard to Self
**




Posts: 50
Registered: 10-4-2015
Member Is Offline

Mood: No Mood

[*] posted on 11-4-2015 at 12:53


ICP-MS ok?
View user's profile View All Posts By User
zephler1
Harmless
*




Posts: 41
Registered: 16-11-2013
Member Is Offline

Mood: No Mood

[*] posted on 11-4-2015 at 13:11


Quote: Originally posted by Lambda-Eyde  
How accurate do you need the analysis? I use a handheld XRF spectrometer (Niton XLp) at work daily and could easily check out your alloy. However it doesn't provide more than one decimal point (I think? It may be two, when I think of it) of accuracy and I'm not sure how accurate it actually is.