midas
Harmless
Posts: 9
Registered: 9-5-2006
Member Is Offline
Mood: No Mood
|
|
Rh bath - cleaning
Do you know of the cleaning of Rhodium bath after jewellery processing?
and I would like to ask also that copper or zinc sweeping from the rhodium bath by the means of the Chramatography?
Best Regards
|
|
enhzflep
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 217
Registered: 9-4-2006
Member Is Offline
Mood: No Mood
|
|
What exactly do you mean midas?
Is your bath contaminated?
If so, best option is to tip down drain or retain for future recycling with (many, many) other such baths.
Platinum has over 200 process from ore to ingot, I'd suspect rhodium to have a
similar or greater number, based purely on it's price (not very scientific, I know)
If you've got 1/2gms per liter, then just forget it for 1L. I know several refiners that
refuse to touch the stuff. They'll refine the gold from such mixtures containing Pt or
Pd, but on a non-industrial scale it's just too much of a headache.
LOL, - I accidently ran reverse polarity one monday morning for 2-3 seconds on a 1 week old bath and our refiner still wouldn't touch it. Shit! There
went $200!!!
You could probably do some form of High Performance Gas Chromotography on a
sample, but IIRC its about $1000 for CSIRO to do something like that.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I'm not saying that nobody would do Gas chromatography on a bunch of metals like Rh, Zn and Cu, I'm just saying that they would only do it to show off
that they could.
Ion chromatography would seem to make more sense if you wanted to analyse the stuff or to purify it (Though I wouldn't like to design the purification
scheme).
Midas, I guess that English isn't your first language. Where are you from?
|
|
midas
Harmless
Posts: 9
Registered: 9-5-2006
Member Is Offline
Mood: No Mood
|
|
Hello my friend; Enhzflep
How are you?
First of all than you for replying my questions and kindly answers,
I am depply interested in refinin rhodium bath. Could you tell me one of refining process that I may use. I have an setting in my mind, for example, I
will use the glass tube, and put into a piece of cotton, and pour the rhodium bath to glass tube through the cotton part. And I am looking for any
chemical solution for holding copper, silver, zinc, gold in the cotton. so finally I have pıre rhodium bath. I am looking just for chemical.
Best regards
|
|
enhzflep
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 217
Registered: 9-4-2006
Member Is Offline
Mood: No Mood
|
|
Hmmm - mmmmmm -mmmmmmmmm.
Yeah, not bad my friend.
No problem.
In a word, no.
The problem is that the rhodium salt present is a rhodium sulfate of some description. In order for the bath to keep plating reasonably bright, one
needs to maintain rather acidic conditions..
Any copper/zinc particles that fall in will be digested, i.e turn into copper/zinc sulfate - in solution ![:(](./images/smilies/sad.gif)
After that monday morning, I too was rather keen to find out how to refine the solution. A number of close associates (all refiners) were not able to
tell me how to do this.
This conversation was some years ago now, and I really don't recall.
From memory you may have some luck using fractional electrolysis. The problem was if I recall correctly, that it is rather difficult to get various
metals to plate out seperately. Not to mention the plating out of the rhodium, or the decomposition of the (purified) rhodium salt without oxidising
the metal.
I'm not aware of a way to precipitate the rhodium from solution in the same way that one may use ferrous(ferric?) sulfate to precipitate gold from
aqua regia.
As I mentioned above, in spite of knowing several refiners personally, I was unable to recover the bath that I ran reverse polarity through that
monday morning - which cost me roughly 1 week's pay at the time.
Although, we did have a black rhodium bath after that...... ![:D](./images/smilies/biggrin.gif)
At ~$700 Aus for 2grams in 100ml solution its not the cheapest stuff to be playing with.
If you manage to find out I'd love to know.
(After that we moved onto Pt plating bath. Is just as good for practical purposes, much, much cheaper, AND you can easily make it yourself )
|
|
midas
Harmless
Posts: 9
Registered: 9-5-2006
Member Is Offline
Mood: No Mood
|
|
Hi!
I did experiments with ferrous(ferric)sulfate. I used hull cell test.
1. old Rh bath
2. old Rh bath +2 g / lt ferrous(ferric)sulfate
3. old Rh bath + amply ferrous(ferric)sulfate
Result :
1. gray and mat
2. white-gray and bright
3. gray and bright
Fe and Rh is plating together aloy. İn your opinion?
You are learned this work.
Now, will I to escape Fe?
Thank you
|
|
midas
Harmless
Posts: 9
Registered: 9-5-2006
Member Is Offline
Mood: No Mood
|
|
Thanks unionised
I will explore ion chromatography.
Yes, English isn’t my first language and my english is bad.
I am from Turkey/İstanbul.
|
|
Texium
|