Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: KBr Beamsplitter
SupaVillain
Hazard to Others
***




Posts: 171
Registered: 28-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-12-2014 at 11:21
KBr Beamsplitter


Okay, so here I am seeing that the traditional preparation of powder FTIR analysis is that it's put into some powdered KBr and mashed with a die, so it makes like a clean lens that the IR beam passes through........

SO WHY DONT WE JUST MASH KBr INSTEAD OF USING CRYSTAL KBr IN OUR BEAMSPLITTERS?!!?!?!?!

Like........ it's not negatively affecting the spectrum or anything because it passes through there anyways.... theres definitely a setup in which the Ge(germanium) can be combined with it, either still deposited onto it as thin film or deposited onto that optical plastic(glass is too opaque) and have the two pressed together.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2736
Registered: 26-1-2011
Location: USA - NC
Member Is Online

Mood: No Mood

[*] posted on 18-12-2014 at 12:17


I am not certain, but think the mashed and compressed KBr forms a glass, not a crystal. Glasses do not have a single crystal structure, so they may not split the beam in the same manner that a single crystal might do. That is certainly the case for silicon, which is a much better semiconductor in certain axises of the crystal, but not as good when melted into an amorphous solid (polysilicon). That is one of the main reasons that PV solar cells are so expensive, as the simpler ones have much lower efficiencies than the ones cut from a single crystal. And complex integrated chips definitely need single crystals.

I am an organic chemist, so my knowledge of solid state and optics is weak. but I know that single crystals are far different that glasses in many ways. Plus I think there are other layers on a beam splitter, but not sure if
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 18-12-2014 at 15:11


I'm not clear on the issue. I do not believe mashing KBr does anything except make the cryx smaller and less uniform. The beam splitter and the KBr pellets do entirely different things. Making a KBr pellet dilutes the material so one can obtain a clear IR spectrum. The KBr doesn't give rise to a spectrum of it's own within the range of the instrument and that's also the reason it can be employed as a beam splitter. I don't know the physics but I believe the beam splitter is a crystal (??). Bob do you know? Or where to look?



"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
SupaVillain
Hazard to Others
***




Posts: 171
Registered: 28-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-12-2014 at 15:26


Well the kbr is just a substrate and so the germanium is the actual beamsplitter, and KBr is opaque because the IR beam is passed through it before it reaches the detector. Thing about crystal KBr is that it is a firm body for a thin film to be deposited onto. The powdered KBr pellet has the same IR spectral transmission range as the crystal, but i think it's all much less structured and it's delicate since it was powder pressed into a disc. But that makes me wonder if powdered germanium or a thin film could be applied to KBr powder and then mixed and stirred up and THEN finally pressed, and come up as the same thing.... i mean i cant think of why that wouldnt work
View user's profile View All Posts By User
SupaVillain
Hazard to Others
***




Posts: 171
Registered: 28-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-12-2014 at 15:33


Of course the beam splitter is a crystal, KBr is the substrate and Ge is the thing actually reflecting some and splitting the beam. But im trying to see if i can make a beamsplitter for cheaper by just using a pellet disc of KBr instead of crystal, and then depositing the Ge film on that or mixing it in to the powder previous to pressing to get the same effect.
View user's profile View All Posts By User
SupaVillain
Hazard to Others
***




Posts: 171
Registered: 28-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-12-2014 at 18:08


Well here in this pic it shows its germanium, not KBr that actually splits the beam, the crystal KBr is only chosen for its ability to be polished down to optical flat grade of flatness and because of its spectrum. Well KBr pellets have the same spectrum and can be pressed to optical flatness as long as there's two optical flats on each side pressing it together.

This might actually be the limiting factor in the capability of making this happen because the top and the bottom flats both have to be level, but maybe i can do some of my own "polishing" with this, that being, making it level to the point in which no point of it is some nm or micron amount higher or lower than any other point

Screenshot_2014-12-18-20-59-28.png - 891kB
View user's profile View All Posts By User
Marvin
National Hazard
****




Posts: 995
Registered: 13-10-2002
Member Is Offline

Mood: No Mood

[*] posted on 20-12-2014 at 14:26


If the KBr was pure, what would keep it as a disc, what stops it from falling apart?
View user's profile View All Posts By User
turd
National Hazard
****




Posts: 800
Registered: 5-3-2006
Member Is Offline

Mood: No Mood

[*] posted on 21-12-2014 at 01:04


Quote: Originally posted by Dr.Bob  
I am not certain, but think the mashed and compressed KBr forms a glass, not a crystal.

Your ideas are intriguing to me and I want to subscribe to your newsletter. :P

Trivial answer: for optical components you want homogeneity. A perfectly homogeneous, anisotropic glass would probably be fine as well, but good luck making one out of KBr.

Moreover, cubic KBr has well defined (100) and (110) crystal faces which conveniently happen to form an angle of exactly 45°.

Quote:
If the KBr was pure, what would keep it as a disc, what stops it from falling apart?

Coalescence.
View user's profile View All Posts By User