Uranium from phosphate ore?
Hi ppl
I can get access to unlimited ammts. of phosphate ore. I know that it contain Uranium (probably phospate, or silicate) to some (very small) extent.
Any ideas hwo to extract it?
I'm very interested in actinide chem.
p.s and no, I'll not try to isolate the 235 isotope.
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
some ideas that poped in my mind...
I guess acidic extraction and then chelating U+n (+3 probably) specie with large organic ligand that solable in dichloromethane or such (the complex
must have very very low decomp. const).
another way can be ion exchange maybe? but I'll still have to seperate it from Ca Mg Fe and other di or tri valent metals
electrochem. is not an option since U has very high red. potintal and very low con.
coments? suggestions?
p.s I appologize for my English. It's not my native lang.
|
|
akinmad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 24-7-2003
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by Dr. Beaker
Hi ppl
I can get access to unlimited ammts. of phosphate ore. I know that it contain Uranium (probably phospate, or silicate) to some (very small) extent.
Any ideas hwo to extract it?
I'm very interested in actinide chem.
p.s and no, I'll not try to isolate the 235 isotope. |
Enrico Fermi's patent no 2708656 gives some insights into leaching of Uranium from uranium ores. HTH
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
thanx for the help, but
sadly , I've calculated in the mean time that actually I'll have to deal
with TONS of the ore since the U conc. there is some ppm. so its impractical even to get mgs. of U that way.
However, I knwo that there are some special steals that contain U as a hardening additive. maybe I should put my efforts this way...
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Hm, never heard of uraniated steel, technetium yes, and thorium (1% or so) in magnesium alloys, but not steel. ???
Tim
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
U're right there is indeed no U in steel, but there is U coated steels in the weapons industry: depleted Uranium
so there is no actual source of U I know about that can be used...
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
If you live in the US, this could be of help.
|
|
praseodym
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 137
Registered: 25-7-2005
Location: Schwarzschild Radius
Member Is Offline
Mood: crazy
|
|
Quote: | Originally posted by Dr. Beaker
Hi ppl
I can get access to unlimited ammts. of phosphate ore. I know that it contain Uranium (probably phospate, or silicate) to some (very small) extent.
Any ideas hwo to extract it?
|
Generally, the ore is treated with a solvent, usually sulphuric acid, to dissolve the uranium compound in the ore. Uranium is then recovered from the
solution by chemical precipitation or by ion-exchange or solvent-extraction methods. Usually uranium oxide is produced, so it has to be reduced to the
metal if necessary.
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
thanks,
I was surprised to find out that U metal is beenig sold freely, however, since I don't live in the US and after 9/11 (which is today, ironically)
I don't think importing it will be good idea )if you see what I mean). so i guess I'll have to try my luck with the ore
|
|
pbmann123
Harmless
Posts: 4
Registered: 30-3-2005
Member Is Offline
Mood: No Mood
|
|
ok well i guess i will post my inquiry here...
i would like to know the most sutable method to produce uranium (u-233, u-235, u-238, all of 'em) from UO2, UO3, U2O5, U3O8. by sutable i mean
the most ecomomically feasable way to produce roughly one kilogram of uranium metal. i have pitcheblende ore of about 38% uranium concentration..
\"Miricle of birth my ass, i\'ll tell you a miricle- birth controle that works\"-stargate sg1
|
|
Jome
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 154
Registered: 10-6-2004
Location: Soutwest sweden
Member Is Offline
Mood: desiccated
|
|
Perhaps the U is unevenly distributed in the ore, like in chunks of pitchblende or something similar. If you have a geiger counter, test the different
minerals found in the ore.
Perhaps aluminutermic reduction followed by removal of resudial Al and Al2O3 by NaOH would work to get U-metal from its oxides?
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
These links may be of use, although I rather suspect that your uranium is in the form of vandates. He is going after radium but alterations in the
methods could give you the uranium you seek.
http://0049606.netsolhost.com/alt/GoingBeyondTheCuries.htm
http://www.nuenergy.org/alt/PerreaultProcess.htm
He is seen by some as a little off in the free energy areas but his chemical methods listed in the links are of use. There is always a grain of salt
to be found if you look.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
If he really thinks you can separate the uranium isotopes chemically he is too far into the left field for my taste.
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Isotopes wasn't the issue, just getting the elements out of the rocks.
|
|
akinmad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 24-7-2003
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by IrC
Isotopes wasn't the issue, just getting the elements out of the rocks. |
In the second link he claims that upper layer of crystals are enriched in lighter isotopose and lower layer is U-238. I am also doubtful about this
statement.
|
|
Dr. Beaker
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 132
Registered: 9-9-2005
Location: between the med red and dead
Member Is Offline
Mood: Shaken, not stirred
|
|
If only life were so easy
then all the difficult and complex centrifugs would be redundent...
and everyone with U deposite will be able to produce enough U235 to create criticle mass (like Iran and other "friendly" countries...)
this is not serious. and if he is mistaken on something so elementery (double meaning ) then I would'nt buy from him used flask.
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
I assumed when I mentioned grain of salt people would see the chemical method he was using and not worry about his whacko science. I have taken radium
from dials and hands and found the chemical method works, as well as playing with uranium, thorium and radium ores. I fail to see why everyone is
getting caught up in his weird science methods and failing to see the very helpful extraction methods. He likely learned these through studying real
science and just can't help adding his own crazy ideas. Surely I am not the only person able to see through the bull and glean some useful
information. If the guy is happy thinking he is seperating isotopes so be it. We don't have to pay attention to that and I would never buy
anything from him either. I will tell you after exaustive searching online and finding little real information as to how to get the radium from my old
hands (several hundred), I never suceeded very well until I got some ideas reading those links. Just ignore the rest of his statements.
|
|
al
Harmless
Posts: 10
Registered: 8-10-2005
Location: France
Member Is Offline
Mood: No Mood
|
|
Uranium from phosphate
"I can get access to unlimited ammts. of phosphate ore. I know that it contain Uranium (probably phospate, or silicate) to some (very small)
extent.
Any ideas hwo to extract it?
I'm very interested in actinide chem. "
In phosphate rocks concentration of uranium is around 100 ppm. Analysis of a sample of the ore must be done , the easiest method is to attack a
sample of mineral, separate uranium via paper chromatography, reagent of uranium is potassium ferrocyanide ( it gives a brown-red color.)
Phosphate rocks have to be heated with 6M HNO3 for 30 minutes, then silicon is volatilized with H2SO4-HF mixture, and the residue is dissolved by a
potassium persulfate fusion.
To extract uranium , two ways :
- acid leaching : H2SO4 and oxydizer
- fusion with carbonate
Choice is made after test experiments.
|
|
akinmad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 24-7-2003
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by akinmad
Quote: | Originally posted by IrC
Isotopes wasn't the issue, just getting the elements out of the rocks. |
In the second link he claims that upper layer of crystals are enriched in lighter isotopose and lower layer is U-238. I am also doubtful about this
statement. |
Sorry bringing up an old thread but when I read a letter from Ernest Glitch (a Victorian scientist and a pal of Faraday) about a Victorian time WMD (a
coal dust flame thrower), I found out very exciting story. ![:o](./images/smilies/shocked.gif)
Mr. Glitch starts mentioning about and describing a victorian time coal dust flame thrower. This is not the thing that puzzles and excites me but he
mentions about his assistant's mental derangement.
Mr. Glitch's assistant talks about a weapon of Uranium which may yield several million tons of TNP .
He does some experiments with Baryte salt they brough from an Expedition to Africa which the assistant claims it contains a special type of Uranium.
![:o](./images/smilies/shocked.gif)
And Mr. Glitch takes him as a mad man and literally thrashes him.
If the accounts stated in that letter is true then I must owe an apology to the guy who mentions about isotope separation by means of barium.
Since jargon used in the letter is Victorian jargon, I did not make it fully so I cannot describe it very clearly.
Please read it yourself : http://www.lateralscience.co.uk/wmd/index.html
P.S. Further reading I was also astonished to see that the assistant mentions about Uranium Halides and gaseous diffusion. ![:o](./images/smilies/shocked.gif)
[Edited on 12-1-2006 by akinmad]
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Ah yes, wonderful stories, unfortunately fictional though.
|
|
akinmad
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 24-7-2003
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by 12AX7
Ah yes, wonderful stories, unfortunately fictional though. |
Yeah it says science fiction. What a fool I'm. ![:mad:](./images/smilies/mad.gif)
[Edited on 12-1-2006 by akinmad]
|
|