Cellulose acetate


How can I make it at home it cant be as simple as vinegar and cotton
View user's profile Visit user's homepage View All Posts By User
trilobite
Hazard to Others
***




Posts: 152
Registered: 25-2-2004
Location: The Palaeozoic Ocean
Member Is Offline

Mood: lonely

[*] posted on 18-2-2005 at 22:08


It takes acetic anhydride to do that.
View user's profile View All Posts By User
kclo4
National Hazard
****




Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline

Mood: No Mood

[*] posted on 18-2-2005 at 22:13


Is there any other way and were can I or how can I get acetic anhydride
View user's profile Visit user's homepage View All Posts By User
AngelEyes
Hazard to Others
***




Posts: 187
Registered: 24-1-2003
Location: South of England
Member Is Offline

Mood: Better than it used to be.

[*] posted on 19-2-2005 at 03:13


Isn't Cellulose Acetate the stuff they use for cigarette filters?

Could be expensive if you're not a smoker though...
View user's profile View All Posts By User
sparkgap
International Hazard
*****




Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline

Mood: chaotropic

[*] posted on 19-2-2005 at 03:15


This thread should be of help.

The only other way is to use acetyl chloride, and trust me, you would do well to stick to the anhydride. ;)

sparky (^_^)
View user's profile View All Posts By User
MadHatter
International Hazard
*****




Posts: 1332
Registered: 9-7-2004
Location: Maine
Member Is Offline

Mood: Enjoying retirement

[*] posted on 19-2-2005 at 17:43
Film


Isn't camera film based on cellulose acetate ?
Just a thought.




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
sparkgap
International Hazard
*****




Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline

Mood: chaotropic

[*] posted on 19-2-2005 at 22:54


Yes, that is true. It replaced cellulose nitrate (Celluloid) for this purpose.

Mylar (PET) is sometimes used.

sparky (^_^)
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 20-2-2005 at 10:48


Transparencies (those clear plastic sheets for overhead projectors) are made of cellulose acetate.



"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to... satisfy any applicable law, regulation or legal process"
View user's profile View All Posts By User
Fluorite
Hazard to Others
***




Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline


[*] posted on 2-11-2020 at 08:48


Can I hydrolyze cellulose acetate to cellulose and acetic acid?
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 2-11-2020 at 13:45


Yes
View user's profile View All Posts By User
Fluorite
Hazard to Others
***




Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline


[*] posted on 2-11-2020 at 21:40


OMG! Really!? We're in Tunisia trying to recycle old cigarettes There's a lot everywhere and I know someone wants to recycle the cotton which is cellulose acetate! He collected a lot of cigarettes in the past 5 months and he asked me to help. if cellulose acetate can be hydrolyze using sodium hydroxide or something we can make ethanol, acetic acid, acetone from cigarettes!

[Edited on 3-11-2020 by Fluorite]
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 3-11-2020 at 07:06


If you would like to produce acetic acid from cellulose acetate by hydrolysis I would recommend acid hydrolysis because

1. Using NaOH will not give you acetic acid, it will leave sodium acetate
2. Cellulose is degraded by aqueous NaOH

By using HCl for example you will end up with acetic acid in solution, with cellulose left behind as it is almost entirely insoluble in water. I'm not sure exactly how you would efficiently make ethanol and acetone though.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 3-11-2020 at 11:46


Quote: Originally posted by njl  
If you would like to produce acetic acid from cellulose acetate by hydrolysis I would recommend acid hydrolysis because

1. Using NaOH will not give you acetic acid, it will leave sodium acetate
2. Cellulose is degraded by aqueous NaOH

By using HCl for example you will end up with acetic acid in solution, with cellulose left behind as it is almost entirely insoluble in water. I'm not sure exactly how you would efficiently make ethanol and acetone though.

I'm fairly sure the acid will hydrolyse the cellulose to glucose at least as fast as it hydrolysis cellulose acetate to cellulose and acetic acid.

It's true that cellulose is degraded by sodium hydroxide, but I think that reaction is typically slower.
View user's profile View All Posts By User
Fluorite
Hazard to Others
***




Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline


[*] posted on 4-11-2020 at 02:51


YO I don't care what happens to cellulose! It's amazing I can make SODIUM FREAKING ACETATE! From cigarette filters!
View user's profile View All Posts By User
Fluorite
Hazard to Others
***




Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline


[*] posted on 4-11-2020 at 02:54


Or I can hydrolyze cellulose acetate using calcium hydroxide to make calcium acetate! And then pyrolyse this to ACETONE are YOu SerIouS! ;D
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 4-11-2020 at 12:03


You can certainly make sodium acetate that way.
Calcium acetate may be more difficult. The solubility of Ca(OH)2 is very low so the solutions are dilute and only react slowly.
It should work, but it will be slow.
Cleaning up the used cigarette neds is a good thing to do, but I find it hard to believe that it's worthwhile compared to adding NaOH to spoiled beer or whatever.

Acid hydrolysis of the filters will give glucose which can be fermented to ethanol, and then to acetic acid.
View user's profile View All Posts By User