Purifying lithium metal


I just received some badly oxidized lithium metal. It is completely black on the outside but inside its silvery. I would like to clean it up.
Can I melt it in some high boiling point mineral oil to melt and remove the oxide layer... Something like that I believe was done to purify sodium - can't remember who. Since lithium melts at 180c ...would it be ok to use mineral oil which boils around 200c?

Also I find that mineral oil is not good for long term storage of lithium. Is there a better oil to preserve lithium metal?
View user's profile View All Posts By User
Oscilllator
National Hazard
****




Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2014 at 03:16


You could do that, but only under an inert atmosphere. Lithium floats on mineral oil (and just about everything else for that matter)
View user's profile View All Posts By User
forgottenpassword
Hazard to Others
***




Posts: 374
Registered: 12-12-2013
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2014 at 04:36


Leave it on. It will protect the rest of the metal from corrosion.
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 21-8-2014 at 04:38


Also be aware that molten lithium can react explosively with glass and many other materials, so I would think twice before doing this. Another way which might clean it up is to put the lithium in an inert solvent and add a small amount of a tertiary alcohol to etch the oxide surface and form the corresponding lithium tert-alcoholate.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8014
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 21-8-2014 at 04:45


I was the one who did this with sodium. With sodium, things, however, are much easier. It melts at low temperature well below the boiling point of water and sodium is more dense than mineral oil. The chance of getting fire or unwanted exposure to air is much smaller with sodium.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 21-8-2014 at 05:06


This thread might be helpful. By the way, congratulations on 5000 posts woelen:D
View user's profile View All Posts By User
jamit
Hazard to Others
***




Posts: 375
Registered: 18-6-2010
Location: Midwest USA
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2014 at 10:03


thanks gdflp for that link!
View user's profile View All Posts By User

  Go To Top