Store lithium
Hi,
For a while I've been storing lithium under mineral oil, the problem is it floats on mineral oil so I made up something to keep it under the oil but
every time I have to deal with the container it's a total mess and i'm kinda pissed off now :p. Is there any kind of oil with a lower density than
Lithium so it doesn't float I can use to store it?
thanks!
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Nope. Search the forum for 'cleaning lithium metal'.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
eidolonicaurum
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 2-1-2014
Location: Area 51
Member Is Offline
Mood: Hydric
|
|
I just put a lump of lead on top of the whole lot. It stays down then, and solves the problem for me.
|
|