Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Ferromagnetic elements and compounds
Pyrovus
Hazard to Others
***




Posts: 241
Registered: 13-10-2003
Location: Australia, now with 25% faster carrier pigeons
Member Is Offline

Mood: heretical

[*] posted on 31-8-2004 at 00:30
Ferromagnetic elements and compounds


How many ferromagnetic elements are there?
In schools they teach that there is only 3; iron, nickel and cobalt, but apparently gadolinium is also ferromagnetic, and as someone mentioned in another thread, so is plutonium(!). All the books I have just list the usual well known ones, which makes me wonder just how many little known ferromagnetic elements there actually are.

[Edited on 31-8-2004 by chemoleo]
View user's profile View All Posts By User
chemoleo
Biochemicus Energeticus
*****




Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline

Mood: crystalline

[*] posted on 31-8-2004 at 02:43


Or to expand this, how many ferromagnetic compositions are there (i.e. oxides, mixtures of metals)?
I know of Fe3O4, and the niob magnets. Anyone?




Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2004 at 02:44


Europiumoxide and chromium(IV)oxide.



One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
Esplosivo
Hazard to Others
***




Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline

Mood: Quantized

[*] posted on 31-8-2004 at 09:43


Interestingly enough certain metal mixtures which possess no ferromagnetic behaviour what-so-ever on their own, become ferromagnetic when they are alloyed. The only such case I can remeber of is a certain mixture of Manganese, Copper, Aluminium and Antimony, although right now I cannot find the % composition of such an alloy.

Ferromagnetism, unlike magnetism, depends on the temperature of the respective alloys, oxides or elements. At a temperature higher than a specific temperature for each of the ferromagnetic substances, known as the Curie point/temperature, the magnetic qualities of such substances vanishes.

It would be also interesting to discuss certain compounds/oxides/alloys with antiferromagnetic properties, such as FeF2, NiO, Cr2O3 and FeCl2 amongst others.

[Edited on 31-8-2004 by Esplosivo]




Theory guides, experiment decides.
View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 31-8-2004 at 10:23


By antimagnetic, do you mean diamagnetic? The most diamagnetic substance is prolytic graphite (only along one axis, though), the most diamagnetic metal is bismuth. Back to magnets, don't forget samarium-cobaltm, alnico (aluminum-nickel-cobalt), and samarium-ferrite.
View user's profile View All Posts By User
Mr. Wizard
International Hazard
*****




Posts: 1042
Registered: 30-3-2003
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2004 at 10:34


Oxygen gas and liquid is ferromagnetic. I haven't tried it, but there was a web site demonstrating the attraction of floating oxygen bubbles in a water bucket being attracted to a strong magnet.
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2004 at 11:19


Oxygen is paramagnetic, not ferromagnetic.



One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1349
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 31-8-2004 at 14:12


There's also all the ferrites - a huge range of materials based on iron oxide combined with other metal oxides like Mn, Zn, Ni.

Garnet is another ferromagnetic material commonly used at microwave frequencies.

Alloys of iron, nickel, molybdemum etc give rise to permalloy, supermalloy, mu metal ... the list is endless.
View user's profile View All Posts By User
Mr. Wizard
International Hazard
*****




Posts: 1042
Registered: 30-3-2003
Member Is Offline

Mood: No Mood

[*] posted on 31-8-2004 at 16:14


Whoops, you are right paramagnet not ferromagnetic for Oxygen. Sometime I see what I want to see.
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 2-9-2004 at 11:53


Ferromagnetic metals are found around the middles of the "d" transition-metal series , and the "f" rare-earth series, of the periodic table, where the numbers of unpaired d and f electrons are greatest. Electrons are added to the d and f orbitals in pairs, with (in the ground state of the metal, but not necessarily in compounds with strong ligands) each orbital having one unpaired electron before the next half of the electrons are added.

This is why Fe, with 5 unpaired d electrons in 5 3d orbitals, is the most strongly ferromagnetic metal of the first transition series (Co and Ni being less so); and why Gd, with 7 unpaired f electrons in 7 4f electrons plus one 6d electron, is likely to be the most strongly ferromagnetic rare-earth metal. Similarly in the actinide series, in which curium would probably be the most strongly ferromagnetic if it could be prepared as the metal in spite of its strong radioactivity. (U, Np, Pu, Am are increasingly ferromagnetic).

Ferromagnetism requires the unpaired electrons (as in paramagnetic substances) to be capable of being aligned with parallel spins in the same direction. By comparison, the elements just before Fe in the periodic table, viz. V, Cr, Mn, are antiferromagnetic, meaning that their d electrons align with parallel but opposite spins, and no bulk magnetism is observable.

In the case of the ferromagnetic Cu-Mn alloy noted above, of which I was previous aware, neither of the component metals themselves being ferromagnetic - I have a sample of it, in the form of an apparently "brass" table light holder that is noticeably magnetic. In the case of this alloy, the d electrons in the conduction band distribute themselves over the atoms of the two metals, approximating to the d electron arrangement of Co. Cu-Fe alloys are likely to be also ferromagnetic, but less so.

Compounds of such metals, like ferrites, magnetite, CrO2, etc. can be ferromagnetic only in the metals' lower valences, with a sufficient number of unused unpaired d or f electrons capable of becoming parallel-aligned. Such compounds are often also electrically conducting, due to some d (or less commonly f) electrons lying in the conduction band.

John W.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 4-9-2004 at 05:31


Esplosivo,
They are called Heusler alloys.
Happy googling
View user's profile View All Posts By User