[*] posted on 23-3-2013 at 03:33
Aluminium carbide Al3C4


Can i make Aluminum carbide by....

Thermal decomposition of sucrose to get some fine Carbon, then powder it, and get some powdered aluminum, heat at 900 degree celsius (Or do i need a higher temperature ?) To melt the aluminum and get Al3C4 ?
View user's profile View All Posts By User
kristofvagyok
National Hazard
****




Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline

Mood: No Mood

[*] posted on 23-3-2013 at 03:39


Quote: Originally posted by KonkreteRocketry  
Can i make Aluminum carbide by....

No.

Metal Al with theor. amount of carbon was heated in elec. furnace at 1975-2000 °C, atmospheric pressure, H2 atmosphere. Yield: 83%
Gmelin Handbook: Al: MVol.B1, 7.5.1.1, page 287 - 290




I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:

"You can’t become a chemist and expect to live forever."
View user's profile Visit user's homepage View All Posts By User
H2libfront
Harmless
*




Posts: 2
Registered: 23-2-2013
Member Is Offline

Mood: No Mood

[*] posted on 23-3-2013 at 05:38


If you have cryolite, maybe you could try this:

"Produces aluminum carbide when the powder metal is heated with carbon at 2000°C or at 1000°C in presence of cryolite"
Source: http://www.hillakomem.com/tag/aluminum
View user's profile View All Posts By User
Hexavalent
International Hazard
*****




Posts: 1564
Registered: 29-12-2011
Location: Wales, UK
Member Is Offline

Mood: Pericyclic

[*] posted on 23-3-2013 at 06:12


Cryolite is also added to the alumina used as a starting material when they electrolytically produce aluminium on an industrial scale, to lower the melting point and reduce costs.



"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
View user's profile View All Posts By User
Adas
National Hazard
****




Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline

Mood: Sensitive to shock and friction

[*] posted on 23-3-2013 at 08:19


This process would need an electric furnace, or induction heater.



Rest In Pieces!