Small crack in retort?
I have a 250ml distillation retort and I was washing it recently and noticed it had a small crack 2 inches in length. Is it still safe to boil things
in, or is there a risk it will shatter and spill every (really bad thing!)?
|
|
kristofvagyok
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 6-4-2012
Location: Europe
Member Is Offline
Mood: No Mood
|
|
Get an oxygen/propane torch and "melt it back".
Elseway it could easily crack when you will heat it up.
I have a blog where I post my pictures from my work: http://labphoto.tumblr.com/
-Pictures from chemistry, check it out(:
"You can’t become a chemist and expect to live forever."
|
|
Nickbb
Harmless
Posts: 25
Registered: 6-12-2012
Location: 3rd dimension
Member Is Offline
Mood: something other than a chemistry pun
|
|
Alright thanks.
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Surround it with Kaowool while it cools.