Author: Subject: white rock polish
michael971
Harmless
*




Posts: 3
Registered: 16-11-2012
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2012 at 12:31
white rock polish


The can has no label. How can I tell if it is tin oxide or cerium oxide?
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 16-11-2012 at 14:46


<a href="http://en.wikipedia.org/wiki/Cerium(IV)_oxide" target="_blank">CeO<sub>2</sub></a> <img src="../scipics/_wiki.png" /> powder is pale yellow.
<a href="http://en.wikipedia.org/wiki/Cerium(III)_oxide" target="_blank">Ce<sub>2</sub>O<sub>3</sub></a> <img src="../scipics/_wiki.png" /> powder is gold-yellow.
<a href="http://en.wikipedia.org/wiki/Tin_dioxide" target="_blank">SnO<sub>2</sub></a> <img src="../scipics/_wiki.png" /> powder is white.
<a href="http://en.wikipedia.org/wiki/Tin(II)_oxide" target="_blank">SnO</a> <img src="../scipics/_wiki.png" /> powder is red or light-tan, may burn in air, or will change to blue-black when heated.

Beyond appearance, try Googling "qualitative tin" or "qualitative cerium".