Synthesis of RhCl(CO)(PPh3)2
ogh for crying outloud!!!
i am having a hard time trying to find the detailed synthesis of RhCl(CO)(PPh3)2 from the literature.
If anybody has any luck finding it, post the reference and how exactly you found it, please.
thanks.
|
|
Polverone
Now celebrating 21 years of madness
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline
Mood: Waiting for spring
|
|
I found it
By searching the literature, of course.
Joseph M. O'Connor and Junning Ma
A High-Yield Conversion of trans-Rh(Cl)(CO) (PPh3)2 to Rh(Cl) (PPh3)3
Inorg. Chem. 1993, 32. 1866-1867
I did a search for your compound formula, exactly as you wrote it, in the JACS electronic search. It seemed to come up in conjunction with
Wilkinson's catalyst and indeed looked much like it. That's what drew my eye to certain articles as being more promising than others.
As you can see from the opening paragraph of the article, Rh(Cl)(CO)(PPh3)2 is formed whenever you use Wilkinson's catalyst to decarbonylate a
substrate. So prepare your Wilkinson's catalyst, apply it to your favorite aldehyde, and recover the Rh(Cl)(CO)(PPh3)2. I've never used
Wilkinson's catalyst, but given the price of rhodium I'm sure a lab exercise using it will have instructions for recovering the
rhodium-containing complex, and you can presumably find such an exercise on your own.
PGP Key and corresponding e-mail address
|
|
Ronald
Harmless
Posts: 1
Registered: 20-7-2004
Location: UK
Member Is Offline
Mood: Sipping Neat Vo
|
|
Ah, so you like Wilkinson's catalyst my boy, very good. Lemme pick out my catalysis and organometallic pamphlets...
GHEY
|
|