Plating silver over copper
which is the best method for plating silver over copper ?
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
the safest way is to make solution of silver chloride, potassiumferrocyanide and boil together with sodium carbonate using a silver anode.i got this
formula from a fellow named Goran Budija at finishing.com
|
|
anoopai
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 51
Registered: 27-11-2005
Location: india
Member Is Offline
Mood: No Mood
|
|
Is this a electroless plating ?, silver anode means just a piece of silver into the solution ?
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
negative this is not electroless plating and yes silver anode means a piece of pure silver as anode(pos).but goran says stainless steel can also be
used for anode. this solution can be used with almost any low voltage and works pretty good.
|
|
Mitchell
Harmless
Posts: 6
Registered: 31-7-2013
Member Is Offline
Mood: No Mood
|
|
I have been looking all over the internet on electroplating silver without the use of AgCN and finally found a recipe. I will be sure to give this a
shot and report my findings. But one quick question what solvent would be used to dissolve silver chloride.
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
i think ammonium hydroxide dissolves silver chloride.
|
|