Calcium Sulfate Hemihydrate
CaSO4-0.5H2O
Can someone please explain how this compound han have half a water molecule as a ligand for water of crystallization?
"Success is going from failure to failure without loss of enthusiasm." Winston Churchill
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
This represents a ratio of molecules in the crystal, ie, there is one molecule of water for every two molecules of CaSO4.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Megak
Harmless
Posts: 12
Registered: 8-12-2011
Member Is Offline
Mood: No Mood
|
|
These numbers are simply molar ratios and are used to make life easier for measuring and theorizing equations. The mole, represents 6.022 x 10^24
representative particles (I think, but you can always look up Avagadro's number). So when there is 1 mole of a substance, you actuallyhave trillions
and trillions of actual molecules or formula units.
I hope this answers your question!
[Edited on 9-1-2012 by Megak]
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Quote: Originally posted by Hexavalent ![](images/xpblue/lastpost.gif) | CaSO4-0.5H2O
Can someone please explain how this compound han have half a water molecule as a ligand for water of crystallization? |
It is 2CaSO4-1H2O, where approximately one molecule of water is shared between two calcium ions and two sulphate ions.
The ratio is not exact and varies between samples.
http://en.wikipedia.org/wiki/Calcium_sulfate#Dehydration_rea...
|
|
bob800
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 240
Registered: 28-7-2010
Member Is Offline
Mood: No Mood
|
|
What would happen if, hypothetically, a single molecule was isolated?
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
There is no such thing as a single molecule in this case. It is a lattice built of calcium and sulphate ions with water molecules shared between them.
Not all substances have exact formulas, some are approximations.
[Edited on 9-1-2012 by ScienceSquirrel]
|
|