Mischmetal coloration - Fe?


I dissolved mischmetal in 1% acetic acid. The iron appears to be quite insoluble at this dilution, so I removed it with a magnet, leaving an almost colorless solution. However, over time, the solution gradually turned orange. Boiling of the solution until crystallization and then redissolution yielded no insoluble matter. I would think that small amounts of Fe were dissolving in the acetic acid, but why did they not precipitate? Also, just about all of the Fe was removed from one vial of mischmetal-acetic acid solution and placed in another identical bottle of solution. The orange color is currently just as intense in one vial as the other.



hibernating...
View user's profile Visit user's homepage View All Posts By User

  Go To Top