fledarmus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 187
Registered: 23-6-2011
Member Is Offline
Mood: No Mood
|
|
Hexanitrohexaazaisowurtzitane
This popped up on one of the blogs I was reading. I wouldn't be surprised if it was already pretty familiar to the high-energy people here, but the
write up was pretty cool! And it was new to me...
Hexanitrohexaazaisowurtzitane
|
|
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1986
Registered: 2-3-2011
Member Is Offline
Mood: No Mood
|
|
You really should have done a google search of this forum before you made this post,
Hexanitrohexaazaisowurtzitane, also known as HNIW or alternatively as Cl-20, has been well described here.
http://www.sciencemadness.org/talk/viewthread.php?tid=3410
You can also read a quick summary of information about he compound on my site:
https://sites.google.com/site/energeticchemical/cl-22
|
|
watson.fawkes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
This article may become significant if only for the first citation of the
phrase "limb-to-chemist ratio".
|
|
killswitch
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 209
Registered: 8-7-2011
Location: is a relative concept
Member Is Offline
Mood: No Mood
|
|
Ha!
But in all seriousness, this PDF from China Lake offers some interesting reading. In it, they mention a viable route to CL-20 with environmental advantages over the
cholorotoluene/benzylamide/Pearlman's catalyst route, and in fact their new route looks like something a garage chemist might actually have a shot at
making.
Anyone want to explore the "limb-to-chemist ratio" of Hexaallylhexaazaisowurtzitane nitrolysis?
|
|
quicksilver
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1820
Registered: 7-9-2005
Location: Inches from the keyboard....
Member Is Offline
Mood: ~-=SWINGS=-~
|
|
CL-20 competes for one of the more expensive energetic materials in private and military industry (@ $1000 per KG in a plant-scale modality and much,
much more in a lab). In fact on a smaller scale is may be the most expensive secondary energetic material in comparative costs ever used (not lab
curiosities). In VERY high end mission critical operations CL-20 (and true ultra pure, consistent size single micron cobalt (and nickel) powder top
the charts of non-radio-active chemical expenditure in Dept. of defense chemical budgetary constraints. The smaller one attempts to synthesize CL-20,
the higher the cost rises! That was why TATB was used in MANY substitution papers & projects.
In comparison PLANT-SCALE synthesis of TATB could be mfg for roughly sixteen cents a pound. High quality HNS, HMX, etc would cost barely 20% more and
due to newer plant techniques, TNT would cost so little, it's till used.
Se: ISEE web site for cost containment of military, industrial energetic materials by yearly basis.
|
|
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1986
Registered: 2-3-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by killswitch ![](images/xpblue/lastpost.gif) | this PDF from China Lake offers some interesting reading. In it, they mention a viable route to CL-20, and in fact their new route looks like
something a garage chemist might actually have a shot at making.
|
So to summarize,
1. allylamine is condensed with glyoxal to form [hexa]allyl- hexazaisowurtzitane. The reaction is apparently very problematic, and they only reported
33% yield. I think the reaction would be much more straight forward, and the yields much higher, if 3-phenylallylamine used instead, because of the
bulky benzene ring groups.
C6H5CH=CHCH2NH2
2. The allyl groups are isomerized by treating with potassium tert-butyloxide in DMSO solvent. No doubt sodium methoxide would work instead, as it is
base catalysed.
R2N-CH2-CH=CH2 --> R2N-CH=CH-CH3
3. The double bonds are simultaneously oxidized, then hydrolyzed off, by concentrated nitric acid, leaving the hexazaisowurtzitane cage nitrolysed.
[Edited on 3-12-2011 by AndersHoveland]
|
|