Looking through the Golden Book of Chemistry Experiments, I found an experiment which involves heating manganese dioxide along with sodium
bisulfate to produce manganese sulfate and sodium sulfate. This, of course, would be extremely contaminated with sodium, so I was thinking of ways to
separate them.
I found another experiment which involved reacting the MnSO<sub>4</sub> with sodium carbonate to precipitate manganese carbonate. I was
wondering if I could filter this carbonate and then react it with sulfuric acid:
MnCO<sub>3</sub> + H<sub>2</sub>SO<sub>4</sub> --> MnSO<sub>4</sub> + CO<sub>2</sub> +
H<sub>2</sub>O
Would this reaction work? It seems to me that it would, but I just want to confirm before I start experimenting.
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
Everything what you said is correct.
|
|
LanthanumK
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Excessive exposure of the carbonate to air may cause it to oxidize.