Hexamine


I took 200ml of 30% formaldehyde solution (Koi Carp treatment) and added ammonia hydroxide solution (says 10% on the bottle but I suspect it is 30%) slowly until I had an excess of ammonia (confirmed by smell).

I then boiled this down and dried it in an oven at 170 deg C.

At some point the liquid turned from clear to yellow as it got to a small volume and then my final hexamine ended up being yellow when wet and light brown when fully dry.

It burns cleanly as it should do but I am wondering if I have contamination or if I have over heated the product and caused the discoloration?
View user's profile View All Posts By User
RustyShackleford
Hazard to Others
***




Posts: 201
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline


[*] posted on 23-3-2025 at 04:26


Probably due to overheating. You can purify it by dissolving it in minimum amount of water and adding acetone to crash it out. acetone should hopefully keep whatever the colored crap is in solution.
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 223
Registered: 25-5-2021
Member Is Offline


[*] posted on 23-3-2025 at 13:14


I'm putting a sample of bought hexamine in the same oven at the same temperature to see if it discolors it. If it doesn't then it must be some contaminant in the formaldehyde.
View user's profile View All Posts By User