Author: Subject: Vanadium
pesco
Harmless
*




Posts: 33
Registered: 19-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 20-12-2024 at 10:01
Vanadium


Hi,
do you guys know of any source of Vanadium ?
I am asking about commonly available items.
Vanadium steel is very poor source with 0.15%-0.25% content.

Please do not reply that I can buy pure V on ebay or somewhere else.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4355
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 20-12-2024 at 10:17


Vanadium(V) oxide is available from pottery supplies. That fact makes it possible for my college to do a lab with the oxidation states of vanadium, as buying reagent grade vanadium compounds is financially out of our budget.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4618
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 20-12-2024 at 11:49


I second that. V2O5 isn’t the most convenient source for doing low valence vanadium chemistry, and certainly isn’t a practical starting point for vanadium metal, but it is the only OTC source I know of if you’re excluding eBay and other online sellers.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Admagistr
Hazard to Others
***




Posts: 371
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 20-12-2024 at 13:02


What about Ferrovanad? I have one that's 80% Vanadium! I wonder how to convert it into a solution as easily as possible? I don't think the acid route is very promising unless I want to work with HF...
There is still a mixture of HCl with HNO3, I don't remember its English name, in our country it is called "Lučavka Královská";-)

[Edited on 20-12-2024 by Admagistr]
View user's profile View All Posts By User
Sir_Gawain
Hazard to Others
***




Posts: 457
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline

Mood: Stable

[*] posted on 20-12-2024 at 13:17


Quote: Originally posted by Admagistr  

There is still a mixture of HCl with HNO3, I don't remember its English name, in our country it is called "Lučavka Královská";-)
In English it’s aqua regia, which is Latin for “royal water”.



“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
View user's profile Visit user's homepage View All Posts By User
Admagistr
Hazard to Others
***




Posts: 371
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 20-12-2024 at 16:20


Quote: Originally posted by Sir_Gawain  
Quote: Originally posted by Admagistr  

There is still a mixture of HCl with HNO3, I don't remember its English name, in our country it is called "Lučavka Královská";-)
In English it’s aqua regia, which is Latin for “royal water”.


In the Czech language it means something like Royal Examiner, Royal Distinguisher. Thanks for the explanation, I'll remember it now, I know a bit of Latin from University, but I've forgotten most of it.

[Edited on 21-12-2024 by Admagistr]
View user's profile View All Posts By User