A decade ago I opened a thread about a chemical way to make calcium.
http://www.sciencemadness.org/talk/viewthread.php?tid=33338
But it is very tedious and still is, so I've given up chemical methods to isolate Ca.
I tried to electrolyze CaCl2 which does release Ca metal at the cathode, but due to the temperature (800 C) it immediately burned away and my cell
made a crackling noise due to the burning of Ca metal. I used a stainless steel pipe end as container and a carbon rod anode and a nickel cathode.
https://www.metallab.net/jwplayer/video.php?f=/forums/CaCl2-...
I was searching on the internet to literature and stumbled upon this
https://www.researchgate.net/publication/365248161_High-temp...
which tells that Ca metal dissolves less in CaCl2 when more CaO is dissolved in the salt bath wich might make the process easier.
Does anyone have experience ?
[Edited on 2024-10-20 by metalresearcher]
|
|
Rainwater
National Hazard
  
Posts: 987
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
Use controlled atmosphere, easiest method is not to blast the reaction with combustion products.
When I switched to all electric heat, problems with my sodium product igniting stopped. It is so reactive at the temperature the hot tourch exhaust
acts as an oxidizer. You dont really need a lot of heating power, just some really good insulation, nice and thick. I shoot for at least 3x as thick
as my reactor is wide of ceramic wool.
"You can't do that" - challenge accepted
|
|
phlogiston
International Hazard
   
Posts: 1381
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
This guy succeeded:
https://www.youtube.com/watch?v=L7X_v4dZEQw
His other video's are worth watching too.
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|