[*] posted on 16-4-2011 at 17:21
platinum coated mesh/wool


Where can I find some platinum coated wool or mesh? I am looking for something to catalytically ignite hydrogen, I would prefer a fine screen but wool would work too if its cheaper. I know these screens/meshes are included in butane soldering irons and liquid fuel hand warmers... Ebay and google turned up surprisingly little, you guys have any tips for me?
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 17-4-2011 at 07:59


Make it. H2PtCl6 onto kaowool and then reduce with H2 gas.



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
beergod
Harmless
*




Posts: 23
Registered: 19-2-2011
Member Is Offline

Mood: No Mood

[*] posted on 17-4-2011 at 22:12


Quote: Originally posted by Fleaker  
Make it. H2PtCl6 onto kaowool and then reduce with H2 gas.


Can you elaborate on how to get the Chloroplatinic acid onto the wool?
View user's profile View All Posts By User
crystalXclear
Harmless
*




Posts: 28
Registered: 30-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 18-4-2011 at 20:03


OOPS..MY BAD.
sorry to misslead, not intentional Xtal

[Edited on 19-4-2011 by crystalXclear]

Kaowool is the ceramic thermaly conductive insulation wool, theres a low conductive paper/wrap form it comes in too IIRC.
it can be used with a hardener as a resin catalyst alternative too. It's been a while and I don't remember much about it, but it's verry safe to use + up to 790-950 degree temps versatility ta boot.

[Edited on 19-4-2011 by crystalXclear]
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 19-4-2011 at 09:52


No, don't electrodeposit.

Make a 0.5 M HCl solution of a known concentration (chloroplatinic acid works for this, but it's an ill defined hydrate often out of the bottle, so just dissolve a mass of Pt into hot aqua regia and then dilute accordingly), dunk the kaowool in, measure the volume loss due to wicking. Take this piece and hang it over the solution with a Pt wire hook until it is drip-dry and load into a quartz tube and reduce at 400*C in a stream of hydrogen.

You can of course tare the dry kaowool before, and then get a mass of Pt deposited.

These plugs work quite nice as heterogeneous catalysts.




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
DJF90
International Hazard
*****




Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline

Mood: No Mood

[*] posted on 19-4-2011 at 10:08


Fleaker, care to elaborate on what Pt/Kaowool can be used for/what you've used it for? And how it compares to other supported Pt catalysts (e.g. Pt/C, Pt/Al2O3)?
View user's profile View All Posts By User
beergod
Harmless
*




Posts: 23
Registered: 19-2-2011
Member Is Offline

Mood: No Mood

[*] posted on 19-4-2011 at 12:10


Any methods not involving a stream of hydrogen gas?
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 20-4-2011 at 08:37


Sure, you can reduce it onto the surface with ammonium formate, at pH 6-6.5 at 80*C. Or you can use methanolic borohydride. Or you can use hydrazine sulfate with ammonia, pH 8, 50*C, amongst others. You can even reduce Pt in solution with hydrogen gas. The best product to be had is that which is prepared in and cooled under a stream of H2, because it's H2 saturated.

Use it as you would any heterogeneous supported catalyst...bearing in mind that it's on an aluminosilicate and those are usually amphoteric. It's best used for continuous flow through catalysis (where Pt/C would erode and Pt/Al2O3 long term phase modifies).




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
Jor
National Hazard
****




Posts: 950
Registered: 21-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2011 at 09:24


I have 5 grams of 5% Pt on Kaowool, commercial sample from BDH. Can I use this in organic synthesis or is it only useful for oxidation of various gasses with oxygen?
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 23-4-2011 at 08:54


You can at least try it. I know it works for hydrogenations.



Neither flask nor beaker.