Striker
Harmless
Posts: 10
Registered: 26-10-2023
Member Is Offline
|
|
Anti-Corrosion Oil Additives
I'm trying to formulate a lubrication blend that's chemically-compatible with polycarbonate. The blend will be based on motor oil and may also contain
automatic transmission fluid (ATF) subject to my ongoing test of ATF's compatibility with PC.
I want to add a corrosion inhibitor to the blend to prevent rust beyond the protection offered by the other components. PC HATES amines and dislikes
cresols, which are common additives for this purpose, so I need to find other options that will play well with both the motor oil (miscible in it if
not liquid) and PC.
Any ideas or insight? I'd like to consider the options before beginning empirical testing.
This is my first post after lurking a while, so please excuse if I'm posting in the wrong place or tripped on a rule.
|
|
Elemental Phosphorus
Hazard to Others
 
Posts: 191
Registered: 11-11-2016
Location: Is everything
Member Is Offline
Mood: No Mood
|
|
Maybe calcium sulfonate might be a good option? It's commonly used as a lubricant thickener and rust preventing agent. I couldn't find compatibility
data on a chart unfortunately, but it seems like it might be better, compatibility-wise than other solvent-y additives like heavy amines and cresols.
Polycarbonate in general, as long as I remember, really doesn't like slightly polar solvents, I believe it can be solvent glued using MEK.
Perhaps calcium sulfonate could work as a corrosion inhibitor?
|
|
B(a)P
International Hazard
   
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
An interesting YouTube video popped up on my feed just the other day about this. You might like to watch this video.
[Edited on 18-11-2023 by B(a)P]
|
|
Texium
|
Thread Moved 19-11-2023 at 09:50 |
Striker
Harmless
Posts: 10
Registered: 26-10-2023
Member Is Offline
|
|
Quote: Originally posted by Elemental Phosphorus  | Maybe calcium sulfonate might be a good option? It's commonly used as a lubricant thickener and rust preventing agent. I couldn't find compatibility
data on a chart unfortunately, but it seems like it might be better, compatibility-wise than other solvent-y additives like heavy amines and cresols.
Polycarbonate in general, as long as I remember, really doesn't like slightly polar solvents, I believe it can be solvent glued using MEK.
Perhaps calcium sulfonate could work as a corrosion inhibitor? |
Thanks for the advice. I came across Calcium Sulfonate in my quest at one point, but sulfonates are esters and I read that PC doesn't like esters.
Maybe I'm misunderstanding or maybe it's not all esters? But yeah, at least it doesn't seem as bad for PC as amines et al.
Maybe I'll buy some to try since you suggest it also.
|
|
Texium
Administrator
      
Posts: 4665
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: Preparing to defend myself (academically)
|
|
It might be fine. “Esters” in that context is probably referring to organic esters used as solvents, such as ethyl acetate. Sulfonate esters are
very different.
|
|
Striker
Harmless
Posts: 10
Registered: 26-10-2023
Member Is Offline
|
|
Ah. Gotcha. Thanks.
|
|