Report on making praseodymium fluoride
This was a simple procedure but being that praseodymium fluoride is probably not often heard about I decided to report.
Atomistry says PrF3 is yellow, but Wikipedia (and supplier info) says green. So I decided to make some. This was my first experiment with a fluorine
compound and I thus proceeded very slowly and in small steps.
The praseodymium starting point was the solution leftover from when I made Pr(NO3)3 and should have had 15g anhydrous praseodymium nitrate in
solution.
Ammonium fluoride NH4F provided the F, with the reaction being a simple double displacement. I acquired the NH4F a few days ago.
6.5g of NH4F was dissolved in 20ml water, I don't think I have ever seen a salt dissolve so fast in water, by the time I completed adding the water
with a squirt bottle it was already a clear solution. This should have put the NH4F in slight excess.
The NH4F solution was slowly added to the Pr(NO3)3 solution under stirring. A light green suspension immediately formed. Stirring was continued for
another 10 minutes and the solution was then gravity filtered.
The remainder was a green wet paste. See photo. This was placed in a desiccator for 36 hours. After this is was bone dry, and basically kept the same
color; maybe a tad lighter. It appears very much the same when viewed in sunlight or fluorescent light.
Dry powder was 10g which was a bit more then the 9.1 aimed for. I suspect there was a bit more then 15g of nitrate in the starting solution or maybe
still a bit of moisture, but it did seem very dry. I decided not to grind it into powder to reduce the chances of breathing in some.
Also attached a photo of the 4 Pr compounds made recently, different shades on green.
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Nicely done. One question though: did you rinse the precipitate in the filter funnel with water a couple times? If you didn’t, there’s a good
chance that your product is contaminated with some excess praeseodymium nitrate or ammonium nitrate.
|
|
Lion850
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline
Mood: Great
|
|
Hi Texium yes rinsed twice in the funnel with copious amount of water. I think all the starting reagents and products apart from the PrF3 is quite
soluble so hopefully the product has little contamination.
|
|